    Hi all I have a new repair project it's a 16ft car trailer.
    Needs some work but price was right. A couple of the 2x4 by3/16 tubing is soft I have pounded away at a few areas and made a few holes. Any problems in cutting out the bad areas and patching in some metal?
    I'd like to save as much metal/ work as I can . I will have to replace several cross members
    Here's a couple of pics the holes are about 1-2" diameter Click image for larger version. 

Name:	image.jpg 
Views:	917 
Size:	142.3 KB 
ID:	12040Click image for larger version. 

Name:	image.jpg 
Views:	945 
Size:	152.0 KB 
ID:	12041

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    If it's rusted out and is load bearing, you should cut out the tubing and replace it, rather than just patching it up. The whole piece could be just as thin from internal rust. Looks like it had water standing in it. With tubing construction, it either has to be 100% water tight, or needs drain holes.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    In addition to drain holes, I swab the inside of non-watertight tubes with cold galvanizing.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4
    Join Date
    Dec 2013
    Location
    Oro Medonte, Ont Canada
    Posts
    9

    Default

    Quote Originally Posted by zoama View Post
    In addition to drain holes, I swab the inside of non-watertight tubes with cold galvanizing.
    Thanks for the advice guys.. Better safe than sorry I had seen some repairs done on a few truck/jeep frames and thought Mmmmm that could work here.. Gonna get cutting tomorrow then order some steel

Similar Threads

  1. Trailer Build Project from Everlast
    By performance in forum Hobyist Projects
    Replies: 12
    Last Post: 07-14-2013, 05:38 PM
  2. Dump Trailer Repair
    By Jake98 in forum Welding Repairs
    Replies: 0
    Last Post: 01-22-2012, 04:10 PM
  3. This is project 1 from zoama585 - 8' x 12' Flatbed Trailer
    By zoama in forum Other Custom Fabrications
    Replies: 0
    Last Post: 09-09-2011, 03:34 AM
  4. Trailer Gate project for 16' trailer
    By chadford in forum Other Custom Fabrications
    Replies: 5
    Last Post: 07-22-2011, 11:15 AM
  5. Boat trailer crank handle TIG weld repair (jakeru's #4)
    By jakeru in forum Welding Repairs
    Replies: 4
    Last Post: 06-18-2011, 07:39 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •