Quote Originally Posted by Mickhd View Post
I switch on welder pp256, set amp to 115, preflow to 1sec,up and downslope,end amps to 45,start to weld ok press switch to stop slops down and stops weld,but the gas is still flowing I have to turn bottle off,also the amps show 45 not 115,and will not adjust,any help out there,the welder is only one month old,iam in uk cheers mick
Are you new to TIG, or just this machine?
AC or DC? 2T or 4T? Also not real clear on your settings, since you grouped amp and time settings together.
Preflow 1 second, you could go a lot lower with that.
Postflow?
Upslope ?
Downslope?
Start amps?
End amps 45
The display will show the actual amps during the weld, if you have end amps set at 45, that is what it will read at the end.