Share
Results 1 to 7 of 7

Thread: Post flow will not stop,and cannot adjust amps just stays on 45

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Post flow will not stop,and cannot adjust amps just stays on 45

    I switch on welder pp256, set amp to 115, preflow to 1sec,up and downslope,end amps to 45,start to weld ok press switch to stop slops down and stops weld,but the gas is still flowing I have to turn bottle off,also the amps show 45 not 115,and will not adjust,any help out there,the welder is only one month old,iam in uk cheers mick

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Mickhd View Post
    I switch on welder pp256, set amp to 115, preflow to 1sec,up and downslope,end amps to 45,start to weld ok press switch to stop slops down and stops weld,but the gas is still flowing I have to turn bottle off,also the amps show 45 not 115,and will not adjust,any help out there,the welder is only one month old,iam in uk cheers mick
    Are you new to TIG, or just this machine?
    AC or DC? 2T or 4T? Also not real clear on your settings, since you grouped amp and time settings together.
    Preflow 1 second, you could go a lot lower with that.
    Postflow?
    Upslope ?
    Downslope?
    Start amps?
    End amps 45
    The display will show the actual amps during the weld, if you have end amps set at 45, that is what it will read at the end.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    I have been welding stick tig flux core,for 40 years,it's the welding set,here are my settings,
    Pre flow 1sec
    Post flow. 45
    Up slope. 5
    Down slope. 5
    Start amps. 45
    End amps. 20
    Tried it in 4t and 2t both the same gas keeps runing
    Tig hf dc on Carbon steel
    Argon pure at 3ltrs per min
    Points 35
    Hope you can help,mickhd

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Mickhd View Post
    I have been welding stick tig flux core,for 40 years,it's the welding set,here are my settings,
    Pre flow 1sec
    Post flow. 45
    Up slope. 5
    Down slope. 5
    Start amps. 45
    End amps. 20
    Tried it in 4t and 2t both the same gas keeps runing
    Tig hf dc on Carbon steel
    Argon pure at 3ltrs per min
    Points 35
    Hope you can help,mickhd
    One thing you can try, instead of turning off the bottle, just turn off the welder and see if the gas stops. If that does it, you might have an ODD gas solenoid problem that has been reported before. Tech support can walk you through fixing the solenoid. As I recall it was also on a multi-function machine, but I don't remember the exact steps to fix it.
    Does this happen just with argon for TIG, or does it also occur when using compressed air for plasma cutting, where the air doesn't stop after the post flow?
    Either way just give tech support a call and they can sort you out.
    Long arc, short arc, heliarc and in-the-dark!

  5. Default

    Cheers Rambozo,I'll give them a ring

  6. Default

    You could have a problem with the pedal or the connection to it maybe too...

    If the machine saw the pedal sw as ON, the gas would flow. Do you hear HF at the same time? I'd unplug the pedal or sw from the machine and see what happens. My 256 did all sorts of weird things just from the connector plug being a little loose!

Similar Threads

  1. no post flow (210 ext)
    By kelly8969 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 02-27-2015, 02:43 PM
  2. New 250EX, low amps, no gas flow
    By Grunbay in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 03-14-2013, 12:28 PM
  3. Power Plasma 50 Post Flow Air Question
    By cpierce18 in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 06-28-2010, 03:02 PM
  4. post flow timer/gas valve?
    By Doug Wright in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 03-22-2010, 08:11 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •