Share
Results 1 to 7 of 7

Thread: help deciding 140st

  1. Cool help deciding 140st

    Hi guys, I've been lurking for a month or so trying to get all the info I can. I'm looking at the 140 or 140st for around my property. It would be used mostly for repairing the iron work fence and gates on the property (some galvanized). As it is over an acre there are many places where i would have to run up to 100 ft of extension for power (10guage with high amp ends). Would the 140 be appropriate for my needs o
    r should i be looking at the 200st? This is of course assuming i can get one in Puert Rico. I see that the shipping policies have changed on the new website. Thanks.

  2. Default

    Sorry so wordy...
    Recap...
    Use: fence and repair at home
    Metal: tube syeel, iromworks some galvanized
    Distance to outlet: up to 100 ft
    Breaker size: 110v 30 amp (could use dryer outlet too)
    welder choices: 140st or 200st (need dual voltage)

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    It depends more on what you are welding. Either machine will be power limited when running on 120 volts, to under 100 amps. If that will do the job for your thickness of metal, then they will do fine. 240 volt power will give you a slightly longer reach with 10ga. cord. This is based on stick welding. For shipping or air freight, the difference in weight, between them, might be a big deal.
    Long arc, short arc, heliarc and in-the-dark!

  4. Default

    The metal is mostly around 1/8" thick. At some points i will have access to a 240v outlet on a 50 amp breaker.
    Others I could reach with the 240v dryer outlet. Some will require 120v, but i figure the material is thin enough that it shouldn't be a problem.
    I'm not very experienced, but given the size of the property, the cost of having someone else do it, and the quality of the work I've had done in the past, I figured I may as well learn a new skill.

  5. #5

    Default

    Shipping policies are the same on the old site. PR, and anything out of the lower 48 are different.

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    1/8" is no problem on 120 volts. The 140 can handle that with ease. As you said, it will probably pay for itself with just a few repairs. Ornamental iron with 6013 or 7014 3/32" electrodes works well. With a little practice, you can just give the welds a quick wire brushing and go right to paint.
    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    Thanks guys. I'm sure I will be here a lot as I work through the learning curve.

Similar Threads

  1. Need some help deciding
    By mliebs in forum TIG Welding (GTAW/GTAW-P)
    Replies: 9
    Last Post: 01-12-2014, 05:32 PM
  2. PA 140ST Received
    By jem5rn in forum Introduce Yourself
    Replies: 3
    Last Post: 01-18-2013, 12:47 PM
  3. Practicing with my 140ST
    By ShaneJackson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-09-2012, 08:01 PM
  4. Help deciding on right TIG/plasma package to purchase
    By sprocket in forum General Welder Questions
    Replies: 40
    Last Post: 04-30-2012, 01:11 PM
  5. Power Arc 140st
    By SeanMurphy265 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 06-16-2011, 11:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •