Share
Results 1 to 20 of 20

Thread: 200dx loosing arc during weld on ac

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default

    Quote Originally Posted by Rambozo View Post
    Is the duty cycle light coming on? Maybe you are exceeding the duty cycle of the machine. What kind of welding are you doing at how many amps?
    Rambozo no lights on and I never went over 140 amp and most of the time was between 90 and 120. Just a side note the digital amp display would drop down to 35 when welding. It would only go up to 120 or what ever I had it set at after I stopped the weld. This may be normal for the machine, I'm not sure.

  2. #2

    Default

    It's normal for the unit to change the reading on the unit to read actual amp output. If it is showing only 35 with the pedal opened up, then there's an issue with the pedal likely.

Similar Threads

  1. How to weld TALL weld beads on 1.6mm thick Aluminum Tube?
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 10-08-2013, 01:49 PM
  2. Buy the Powertig 200dx or save for The Dynasty 200dx
    By AfroPaul in forum TIG Welding (GTAW/GTAW-P)
    Replies: 40
    Last Post: 05-13-2013, 07:18 PM
  3. Poor weld quality on my 200DX. Need help.
    By RDK_YJ88 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 01-24-2013, 11:42 AM
  4. Penetration of weld and weld build up?
    By CGCINC in forum General Welding Questions
    Replies: 4
    Last Post: 07-03-2012, 07:06 AM
  5. Will Powertig 200dx weld aluminum cans and razor blades ?
    By bnun12 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 06-11-2012, 12:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •