Thread: Power ultra205p plasma settings?

  1. #1
    Join Date
    Dec 2013
    Location
    Oro Medonte, Ont Canada
    Posts
    9

    Unhappy Power ultra205p plasma settings?

    Click image for larger version. 

Name:	image.jpg 
Views:	338 
Size:	136.1 KB 
ID:	11995Hello all I have a pu205p pretty new (dec13) have only used the plasma function once before today and that was on some very thin metal. Today I was looking to cut some 1/2" ,the specs say the machine will do 5/8" severance and 1/2" cuts part of reason I got it. Well when set it up to cut I was not getting a good cut at all as a matter of fact it didn't even go through the metal..I did cut the same metal with another plasma Hobart Awhile ago and it was pretty quick. You can see in the pics the Hobart cuts straight and cleanand the pu205p cuts don't seem to get the penetration..
    I altered my air pressure from a low of 60 ish to high 70 psi. I have a 60 gallon compressor with air dryer and a second air dryer at the unit..my amps are set to max 49.. Suggestions? I really don't want to grind the metal out...Click image for larger version. 

Name:	image.jpg 
Views:	327 
Size:	131.8 KB 
ID:	11992Click image for larger version. 

Name:	image.jpg 
Views:	406 
Size:	140.0 KB 
ID:	11993Click image for larger version. 

Name:	image.jpg 
Views:	406 
Size:	140.0 KB 
ID:	11993[/ATTACH]Click image for larger version. 

Name:	image.jpg 
Views:	344 
Size:	150.0 KB 
ID:	11994

  2. #2

    Default

    You may not have your work clamp connected right. Do you have it in the negative or positive? Have you checked your consumables and made sure they are tight and the swirl ring is mounted correctly?

  3. #3
    Join Date
    Dec 2013
    Location
    Oro Medonte, Ont Canada
    Posts
    9

    Default

    Well I checked all fittings consumables etc all good, I bumped up the air pressure a smidge or two and made some pretty good cuts.. Seems like my rate of travel was the biggest culprit and possibly the ground. Thks for suggestionsClick image for larger version. 

Name:	image.jpg 
Views:	370 
Size:	134.6 KB 
ID:	11999Click image for larger version. 

Name:	image.jpg 
Views:	370 
Size:	134.6 KB 
ID:	11999Click image for larger version. 

Name:	image.jpg 
Views:	358 
Size:	134.0 KB 
ID:	12000Click image for larger version. 

Name:	image.jpg 
Views:	370 
Size:	142.4 KB 
ID:	12001Click image for larger version. 

Name:	image.jpg 
Views:	333 
Size:	142.3 KB 
ID:	12002

Similar Threads

  1. Power Plasma 60, 60S, 60C?
    By Zoomie in forum Everlast Plasma Cutters (PAC)
    Replies: 10
    Last Post: 11-16-2013, 12:24 AM
  2. Power Pro 205 Pulse Settings
    By Ray C in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 09-17-2012, 02:49 AM
  3. Power Plasma 50 plasma cutter....
    By CGCINC in forum Customer Testimonials
    Replies: 4
    Last Post: 07-20-2012, 12:58 PM
  4. My Power Plasma 50
    By jtybt in forum Everlast Plasma Cutters (PAC)
    Replies: 27
    Last Post: 04-28-2010, 08:08 PM
  5. Plasma Cutting Settings Super 200P
    By CapnMilo in forum General Welder Questions
    Replies: 3
    Last Post: 02-05-2009, 07:48 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •