These are mine. I only changed HF start duration (D02, was ~2.0) and DC start amps (D04, was ~30). Everything else is factory default.
D01= N/A {00.5)
D02= HF Arc start duration (.5-5 seconds) {5.0}
D03= HF Arc start frequency (10-100Hz) {50}
D04= HF Arc start amps DC (10-100 amps) {10}
D05= HF Arc start amps AC (15-100 amps) {40}
D06= N/A {1.5}
D07= Lift start current DC and AC (10-100 amps) {15}
D08= Torch trigger or amp control 4T function by type torch (00 = 4T 01 = 4T Normal) {00}
D09= Voltage Reduction Device for MMA/stick (00 = VRD off 01 = VRD on) {00}
D10= Pulse mode Standard or Advanced. AC is added to DC in Advanced mode (00 = Standard 01 = Advanced) {01}




Reply With Quote