Share
Results 1 to 7 of 7

Thread: Convert Welder to Gas-Thru DINSE?

  1. #1
    Join Date
    Dec 2013
    Location
    Chandler, Arizona, USA
    Posts
    85

    Default Convert Welder to Gas-Thru DINSE?

    Another crazy idea here…

    I find myself moving between my 210EXT and a Lincoln 225 often - I'd like to use my CK torch on both, without changing the QD fitting. The 210EXT uses a separate gas connector at the welder, while the Lincoln uses a gas-thru fitting.

    I'm wondering if anyone's converted the DINSE outlet on their welder to gas-thru, and what issues might emerge. What happens when a stick is is connected to the same DINSE? Is a gas-thru DINSE longer to push the coupler open?

    ASSuming there's enough room in the case, it'd seem to require changing out the DINSE fitting and moving the gas connection to it. Is there a good source for the fitting?

    Plan B would be to hack together an external adapter to do the same. CK has a power hose extender that could do it, but it's 12' long.

    Cheers,
    Richard
    210EXT (2013 USA)

  2. #2

    Default

    Well... Slightly more expensive, but why don't you buy another torch so each machine will ready to go?

  3. #3
    Join Date
    Dec 2013
    Location
    Chandler, Arizona, USA
    Posts
    85

    Default

    Quote Originally Posted by broberts5 View Post
    Well... Slightly more expensive, but why don't you buy another torch so each machine will ready to go?
    The second welder is at a shop that I use. It's got a torch, but I wouldn't mind using my FlexLoc with it. Toting my torch back and forth is tolerable, but buying another FlexLoc kit just to use there probably doesn't make sense.

    It seems that gas-thru DINSE is the most compact option, so finding a way to adapt to it as common ground seems to make sense. Either by converting the welder's outlet, or simply making a short hose extension with the different ends, and having the torch have just the one common fitting.

    Cheers,
    Richard
    210EXT (2013 USA)

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Converting it sounds like the best way to go. I have also been looking for panel mount gas through DINSE, and so far the only thing I know of is to order it as a repair part from Lincoln or Miller. If you find another source, please post it.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5

    Default

    Like the last 4 at the bottom of the page http://weldingdirect.com/connectors.html search for gas. Man they are expensive.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by everlastsupport View Post
    Like the last 4 at the bottom of the page http://weldingdirect.com/connectors.html search for gas. Man they are expensive.
    Nope, we are both looking for the panel one to go on the machine. Torch male is everywhere, but the panel female is damn scarce.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Quote Originally Posted by Rambozo View Post
    Nope, we are both looking for the panel one to go on the machine. Torch male is everywhere, but the panel female is damn scarce.
    Wonder why? Mating of the gas line and leaking maybe? Will look again. You said L and M had them.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Convert Harbor Freight 20 ton press to 32 ton
    By Steve in forum Other Custom Fabrications
    Replies: 62
    Last Post: 06-04-2013, 03:29 AM
  2. Replies: 11
    Last Post: 10-15-2011, 04:29 PM
  3. Anyone know how to convert a cordless drill to corded?
    By Mikeymetal in forum Personal Projects (no welder required)
    Replies: 20
    Last Post: 05-07-2011, 01:21 PM
  4. convert powerI tig to AC/DC?
    By iil in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 12-03-2010, 09:07 PM
  5. Convert program for Windows
    By rengaw21001 in forum Technical Bulletins and Tips
    Replies: 0
    Last Post: 11-07-2010, 11:00 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •