I'm certainly no expert at this but, it seems to me that if it "builds too much heat in the weld area and then drops out" you're using too much current (maybe to compensate for the "cold" condition of metal at the beginning of the weld). If the amps were set right for the "built-up heat" then the preheating at the start would make the material ready for that setting from the begining...

No?