I have a 200DX and I've been welding a fair amount of chrome moly tubing.

The problem I'm having is in adjusting the pedal.

The gain knob on the front of the pedal when turned up doesn't allow me to back off the amperage enough to allow my crater to cool and move without loosing the arc. If I turn it down so I can basically just keep a light pilot arc going to see and move then I don't have the amps I need to heat the base metal quickly.

My gain knob usually is set at about 7 or almost all the way up, it is very touchy.

I'm using 5/32 tungsten 2% lanthanated sharpened to a point, Argon gas.

Right now I'm kind of band aiding the situation by running my post flow up a little and using that to keep my low amperage arc going.

The machine is very stable except for the foot pedal do I have something setup wrong?