  1. Default New MTS 250S 802 Error

    I bought an MTS250S from Amazon this week. I live in Florida Keys so Amazon Prime is my best friend. Received it on 2/19. Unboxed and hooked up stick. Set AF to 50 and current to 130. Welding 3/8" plate with 1/8" 7018. Upon striking stick on plate, welder would stop functioning and amber light comes on with 802 displaying in window. Only way to try again is to cycle power. I called Everlast and left message. A nice fellow named Ray I believe called me back and said no love, send it back and get replacement. Got replacement yesterday and did same procedure with same settings. Same problem. Could Amazon have bad batch? Sent tech@everlastwelders.com and email for advisement. Also front bezel cracked all over (see attached). UPS isn't always the most gentle with their packages. Any feedback appreciated. Need welder to perform as expected. This unit was $1500 on Amazon.

    Click image for larger version. 

Name:	bezel_cracked.jpg 
Views:	510 
Size:	143.5 KB 
ID:	11804

  2. #2

    Default

    If you you are sticking the electrode on the plate, it is possible that it will do that, especially if more than 1 seconds. What are your settings? Are you using EP? On the cracked bezel, I dont' think I've seen one on an MTS. That is definitely something you need to remedy with Amazon.

    Also have you checked your input power across the terminals? What is your power source? Are you by chance using a generator?
    Last edited by performance; 02-23-2014 at 01:48 PM.

  3. #3

    Default

    Welcome to the forum colddainhell.
    Cant realy answer your question.
    Lincoln A/C 225
    Everlast P/A 200

  4. #4
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Colddainhell, Welcome to the forum sorry to hear your having a problem with your MTS250S and getting a cracked case also. I have a MTS250S also and did have the code 802 also with a little help from the Everlast team I did get it fixed I love the MTS250S, hope it is something simple.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  5. Default

    Thanks Kempy. Glad to hear you like it. What was your issue? Do you have a link to your thread?

    Performance, as far as settings go, I set AF to 50 and current to 130. Welding 3/8" plate with 1/8" 7018 rod. Watched Jody do his review and set AF at 77. No dice. As soon as I drag the rod, I get a little spark and then nothing but amber light. I don't even get the chance to get the rod stuck. I am plugged into same plug that normally has a XMT 300cc running fine, so I know its not the shop. Yes its EP. How do I check input power across terminals? BTW guys thanks for any assistance. Going to try Tig and Mig tonight to see if that is affected.

  6. #6
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    http://www.everlastgenerators.com/fo...highlight=code

    Colddainhell this the link to the problem I had they did change the machine it was one of the first machines that Everlast got in Canada but it would weld it never stop altogether and I did not try stick with it. You are on your second machine with the same problem hard to believe that you would get two with the same problem did you check to see if they sent you back the same machine again. The MTS250S is a very nice machine the Mig weld like a Tig in steel and aluminum when you get it set up right. You will find job I have put on the site.
    Last edited by Kempy; 02-23-2014 at 06:49 PM. Reason: ADD
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  7. #7

    Default

    It DOES matter. An XMT has power factor correction and can handle lower voltage and dirty power supply. It makes a huge difference. To measure power input, you simply stick the prongs of your Volt meter into the two hot legs of the receptacle... preferably with one hand for safety and do it at your own risk.

  8. Default

    Mark. Attached is the voltmeter reading from the outlet. It was steady at 240 for the whole time. What should I try next?

    Click image for larger version. 

Name:	voltmeter.jpg 
Views:	480 
Size:	123.5 KB 
ID:	11809

  9. Default

    I still have the original machine and the second machine. I measured the voltage like Mark asked.

  10. #10

    Default

    Have you tried a smaller rod? Lower amps? Lower Arc force? If so, what is the threshold where it won't do it (if it won't) Just trying to isolate possible causes and improve our chances of being able to get this resolved without any more back and forth shipping. Have you tried any other processes? I would also look really good at the ground. Are you using the standard leads/lengths sent with the unit?

  11. Default

    I will try lower AF and amps. Only have 1/8" 6010 and 7018 right now.

  12. Default

    After trying the Mig and Tig functions with same problem. I found the source of the overloading. Apparently the bezel in the rear with the fan was also damaged during shipping and the fan bracket/housing is broken. I did not notice this until hooking up the gas cylinder. The fan does not even spin up. I am going to return both and try to get one that can be shipped with out taking a ground and pound from UPS.

    Click image for larger version. 

Name:	broken_fan.jpg 
Views:	492 
Size:	145.4 KB 
ID:	11810

    Thanks for everyone's help.

  13. #13

    Default

    Perhaps the machine has a safety cutoff that prevents it from running if the fan isn't spinning. Either way, I wouldn't accept either unit given the cosmetic (and who knows what else) damage.

  14. Default

    I finally received an Everlast MTS250S from Amazon that did get beat up by Mike Tyson. I am happy to report that all functions are working as expected. I do have one question as to the difference between a Mig 15 and Mig 25 torch. The first and second machines came with a Mig 25 and the third came with a Mig 15. The torch looked smaller. Can anyone shed any information?

  15. #15

    Default

    Quote Originally Posted by colddainhell View Post
    I finally received an Everlast MTS250S from Amazon that did get beat up by Mike Tyson. I am happy to report that all functions are working as expected. I do have one question as to the difference between a Mig 15 and Mig 25 torch. The first and second machines came with a Mig 25 and the third came with a Mig 15. The torch looked smaller. Can anyone shed any information?

    It should have 25 or 24 series...definitely not a 15. 15's are good for a max of 180-200 amps.

  16. Default

    I don't want to send this whole unit back. I am assuming the packaging department made a mistake? Can Everlast ship me the correct torch?

    Click image for larger version. 

Name:	mig15torch.jpg 
Views:	498 
Size:	143.9 KB 
ID:	11846

  17. #17

    Default

    You'll have to call Everlast directly to discuss it.

  18. #18
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by colddainhell View Post
    I finally received an Everlast MTS250S from Amazon that did get beat up by Mike Tyson. I am happy to report that all functions are working as expected. I do have one question as to the difference between a Mig 15 and Mig 25 torch. The first and second machines came with a Mig 25 and the third came with a Mig 15. The torch looked smaller. Can anyone shed any information?
    Nice to see you got everything sorted out with the MTS250S now you can do some welding good luck with it I like mine was using it today welding a titanium exhaust pipe for a guy that cut a hole in it with a torch trying to take the valve out of it.

    Click image for larger version. 

Name:	titanium Exhaust Pipe.jpg 
Views:	490 
Size:	135.4 KB 
ID:	11848
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

Similar Threads

  1. Weekend trial and error on a 250EX. Warning long winded beginner!
    By Tommy Coates in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 08-02-2015, 09:36 PM
  2. 255ext Error E02
    By labmaster02 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 06-29-2015, 04:23 PM
  3. MTS 250S Features Usage
    By colddainhell in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 4
    Last Post: 03-29-2014, 12:27 PM
  4. New Videos for the PowerMTS 250s
    By performance in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 14
    Last Post: 04-30-2013, 01:11 PM
  5. website error?
    By eventhorizon in forum Forum related Questions
    Replies: 2
    Last Post: 03-03-2011, 10:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •