    Hi, all.

    Well, I spent the weekdays getting prepped with scrap metal, gas, consumables, etc., and left the best 'till last... wiring the plug and powering up my new unit. Sadly, no joy.

    I get a light in the rear power switch, but no fan action or front panel lights. Maybe I'm overlooking something, like a second switch?

    Is there a user-servicable fuse / breaker inside, or is it time to contact tech support?
    210EXT (2013 USA)

  2. #2

    Default

    Post a pic of how you wired the plug (inside the plug pic).
    Did you check the voltage at your outlet ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    Dec 2013
    Location
    Chandler, Arizona, USA
    Posts
    85

    Default

    Thanks for the quick reply.

    Yup, the outlet's good; it's been feeding my compressor for years. I've verified power's good into the unit, so it's looking like an RMA...
    210EXT (2013 USA)

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I put it in the wrong thread, so I will repost here. The color code on the power cord is a bit unconventional since this can be wired for single or 3 phase. I noticed the manual also doesn't have the nice diagram for the plug that you will find in the 250EX manual. Be sure you are not using the red wire for single phase operation.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5
    Join Date
    Dec 2013
    Location
    Chandler, Arizona, USA
    Posts
    85

    Default

    Quote Originally Posted by Rambozo View Post
    The color code on the power cord is a bit unconventional since this can be wired for single or 3 phase. I noticed the manual also doesn't have the nice diagram for the plug that you will find in the 250EX manual. Be sure you are not using the red wire for single phase operation.
    Thanks! This unit is single-phase only, so you can't wire it wrong unless the green wire isn't ground. But for everyone's peace of mind, here's a photo:
    Click image for larger version. 

Name:	210 EXT Plug.jpg 
Views:	449 
Size:	89.1 KB 
ID:	11531
    G=green
    X=black
    Y=white
    Plug is an L6-30P (240v 30A, locking)
    Last edited by RichardH; 12-29-2013 at 05:10 AM.
    210EXT (2013 USA)

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Nevermind. I'm out of date again.
    Last edited by Rambozo; 12-29-2013 at 05:19 AM.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by RichardH View Post
    Thanks! This unit is single-phase only, so you can't wire it wrong unless the green wire isn't ground. But for everyone's peace of mind, here's a photo:
    Click image for larger version. 

Name:	210 EXT Plug.jpg 
Views:	449 
Size:	89.1 KB 
ID:	11531
    G=green
    X=black
    Y=white
    Plug is an L6-30P (240v 30A, locking)
    I use the same plugs and receptacle did you check the voltage.
    Click image for larger version. 

Name:	plug.jpg 
Views:	393 
Size:	129.1 KB 
ID:	11532
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  8. #8

    Default

    Quote Originally Posted by RichardH View Post
    Thanks for the quick reply.

    Yup, the outlet's good; it's been feeding my compressor for years. I've verified power's good into the unit, so it's looking like an RMA...
    The first step is to call tech support monday morning. He'll walk you through troubleshooting. If that doesn't get it working he'll issue the RMA.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9
    Join Date
    Dec 2013
    Location
    Chandler, Arizona, USA
    Posts
    85

    Default

    Quote Originally Posted by zoama585 View Post
    The first step is to call tech support monday morning. He'll walk you through troubleshooting. If that doesn't get it working he'll issue the RMA.
    Cool, thanks. I was hoping I missed something obvious, but it doesn't seem like it. Will-do.

    Cheers,
    Richard
    210EXT (2013 USA)

Similar Threads

  1. A Dumb Question About the PT210EXT
    By DaveK in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 06-02-2015, 07:52 PM
  2. dumb dens connector question
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 04-27-2011, 07:58 PM
  3. Dead on Arrival
    By timtunks in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 02-25-2009, 11:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •