    Default TIG - Practicing beads on mild steel, getting a bump at the end

    Oooo, when will the winter lighten up
    Well, I can practice welding

    I'm practicing beads. This is 1/4 mild steel. Filler is 1/16 ER70S6, and tungsten is 3/32 2% ceriated. Machine is an analog iTig 200. I've got a foot pedal. Post flow is around 2:00 (scale of 0-25 might put that around 12 seconds), and down slope is set to 1 (on a scale of 0 to 5). I'm left handed so the torch goes from left to right and I end on the right. I'm ending up with a bump at the end of the bead. I've tried changing a few things but haven't really figured out what makes this better or worse. Maybe someone else has. I've put in the standard dime size benchmark.

    While I've got ya looking, how am I doing? I know some of these are too flat, and I'm learning more about what happens as the base material soaks up more heat. Are some of these beads at least halfway decent? I've been a hobby welder long enough to figure out there's a lot more I still need to figure out! I have read in other postings mild steel beads should look at least a little shiny, but the only time I get anything shiny is when tack welding.

    Thanks in advance for your time and tips.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	beads1.jpg 
Views:	539 
Size:	70.5 KB 
ID:	11778   Click image for larger version. 

Name:	beads2.jpg 
Views:	497 
Size:	88.0 KB 
ID:	11779  
    Sean M
    Illinois
    I-Tig-200 (March 2012)
    Harbor Freight 90 Amp Flux core Mig
    (Sold this one but I might have picked up some bad habits -->) Harbor Freight 130 Amp lift-start Tig (the red one)

  2. Default

    Maybe set your down slope to 3 or 4 and try that.

    Or set your down slope to 0 and just back off the pedal slowly at the end of the run.

    And what flow rate are you running on the argon?
    From the desk of Kevin Caron, where the answers are stranger than the questions....

    www.kevincaron.com

  3. #3

    Default

    Hey Kevin. I appreciate and enjoy the videos you've put out there. Thank you for the time you put into that. I'll try both suggestions on the down slope & foot pedal. Flow rate is at 6 LPM. The torch is a CK 9 flex with the gas saver and a 5 cup. I believe the CK information says to set the flow at 4-5 for this size cup. I've tried 4 through 6 LPM and maybe even higher flow rates, but don't seem to get the weld looking any less dull.
    Sean M
    Illinois
    I-Tig-200 (March 2012)
    Harbor Freight 90 Amp Flux core Mig
    (Sold this one but I might have picked up some bad habits -->) Harbor Freight 130 Amp lift-start Tig (the red one)

  4. #4

    Default

    Check your preflow and postflow. Increase it as much as you can.
    The beads are fine. It's hard to make beads on a flat plate look good. Likely it is your torch angle or gas flow rate that may be an issue. You aren't going to get a mirror finish typically unless you wire brush it. A gas lens helps.

Similar Threads

  1. Welding 1/8 to 3/16 mild steel with powerarc 140st on 120v ?
    By ridenlow559 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 02-15-2015, 02:58 AM
  2. Filler metal selection for welding mild steel and 4130 tube
    By hooda in forum General Welding Questions
    Replies: 11
    Last Post: 03-21-2013, 08:38 PM
  3. Been practicing on some aluminum...
    By blasphemy000 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 11-12-2012, 02:19 PM
  4. Practicing with my 140ST
    By ShaneJackson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-09-2012, 09:01 PM
  5. Welding Stainless to Mild...
    By CGCINC in forum General Welding Questions
    Replies: 4
    Last Post: 01-28-2012, 07:07 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •