Unless, like me, you only have a DC machine, then you have to work with what you have. also, just another option to try, maybe if you are just curious and like to try different methods, dont have helium, have a stick machine converted to TIg, etc.... Like I said - just want to open a discussion for those that like to / have to / think outside of the box.