    Purchased a water cooled torch, not that I'll use it that much with the PP 205 but I really like how small the WP-20F is. Came up with my version of the tap water system that works great. Pics are of the welder connections, the shop sink water source, backyard drain and I threw in one of my tig finger holder. Someday maybe a real cooler but this is just fine for now. Click image for larger version. 

Name:	cooler hoses.jpg 
Views:	1181 
Size:	140.2 KB 
ID:	11708Click image for larger version. 

Name:	drain.jpg 
Views:	1218 
Size:	147.2 KB 
ID:	11709Click image for larger version. 

Name:	water hose.jpg 
Views:	1227 
Size:	141.9 KB 
ID:	11710Click image for larger version. 

Name:	601 tig finger.jpg 
Views:	1240 
Size:	142.0 KB 
ID:	11711

  2. #2

    Default

    Nice...I like the drain.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    There you go.
    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    If nothing else you get a little heat in the pool too. Slick.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    Are you running argon through the water trap/pressure regulator on back of the machine ?.. It's looks that way in the pic. Argon should go from your flowmeter directly into the machine.
    Last edited by zoama; 01-16-2014 at 07:20 PM.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6
    Join Date
    Oct 2013
    Location
    Glendale Arizona
    Posts
    26

    Default

    Are you running argon through the water trap/pressure regulator on back of the machine ? Zoama, That only happens when I forget to turn that shutoff, there are 2.

  7. #7
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I see you have a GM weather pack connector at the front of the machine looks like it is going to the control plug what is that for? Nice work on the plumbing.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  8. #8
    Join Date
    Oct 2013
    Location
    Glendale Arizona
    Posts
    26

    Default

    Click image for larger version. 

Name:	2 pin connector.jpg 
Views:	1042 
Size:	146.0 KB 
ID:	11728Kempy, I had some of these 2 pin weatherpac connectors and no 7 pin plugs for some new torches. I did the cheap way out for the new ones. It actually works just fine.

Similar Threads

  1. tig cooler
    By postmark in forum Welding Projects and Pictures
    Replies: 1
    Last Post: 01-07-2015, 12:26 AM
  2. Tig cooler cooler power source - "warning"
    By Odyknuck in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 12-17-2012, 09:37 PM
  3. TIG 200DX Alternative Pedal Option
    By compression in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 04-18-2012, 06:12 PM
  4. Replies: 28
    Last Post: 03-29-2012, 05:16 AM
  5. Alternative tig torch selecton for pp205
    By rodjava in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 01-04-2011, 07:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •