Purchased a water cooled torch, not that I'll use it that much with the PP 205 but I really like how small the WP-20F is. Came up with my version of the tap water system that works great. Pics are of the welder connections, the shop sink water source, backyard drain and I threw in one of my tig finger holder. Someday maybe a real cooler but this is just fine for now.