    I think I have lost some of the range on the balance and cleaning on my 250 EX.
    It used to adjust to a very high pitch. Now, once I get to 30% cleaning and 200 on balance
    I do not notice any change in pitch, if I continue to adjust it. Ant tips on how to verify this?
    Thanks

  2. #2

    Default

    Quote Originally Posted by broberts5 View Post
    I think I have lost some of the range on the balance and cleaning on my 250 EX.
    It used to adjust to a very high pitch. Now, once I get to 30% cleaning and 200 on balance
    I do not notice any change in pitch, if I continue to adjust it. Ant tips on how to verify this?
    Thanks
    Balance doesn't affect pitch. Frequency does.

  3. #3

    Default

    Thanks. My bad. My real problem is that my tungsten is splitting. Doesn't matter much what amps. That's why I thought it might be frequency or cleaning. Any thoughts?

  4. #4

    Default

    Too much cleaning can cause issues. It's going to depend upon the tungsten. What type are you using? Red can split occasionally with too high of cleaning. It can be caused by low quality tungsten as well.

  5. #5

    Default

    I'm using 3/32, 2% thoriated, lanthanated, ceriated. Have used them all. It used to keep a nice point. Now it won't. My settings are: frequency-200, cleaning 20-30%.

  6. #6

    Default

    ...even if I turn frequency all the way to 250 and cleaning to 10% it won't keep a point.

  7. #7

    Default

    200 and 250 hz frequency? Why would you want that? 100-150 hz is sufficient for 99.5% of all welding. It's likely you are putting too much stress on the tungsten running at that extreme. You could be putting too much heat too for its size.

  8. #8

    Default

    Thanks. I'll test that out. I guess I got greedy! I like a narrow bead with very little etching.

  9. #9

    Default

    I ran some beads with the freq set at 100 then 150. That gives me a very wide etching. It seems that I've lost the perceived advantage of the inverter. I do a lot of cosmetic aluminum for show cars. Things like al radiators. It's an advantage to minimize the etching. 100-150 freq and 30% cleaning don't do it. HELP!

  10. #10

    Default

    Drop it to 20%. But etching is a result of AC+ and TIME. If you are getting too much etching at a reasonable frequency (twice that of a transformer at least), you are going too slow, and/ or not using enough amps.

    It can also be from too much standoff and torch angle. Do you have a penny's or quarter's thickness under the tungsten?

  11. #11

    Default

    I think it'd be easier if you could give us some parameters so we can weed out multiple possibilities.
    What metal thickness/type?
    Tungsten thickness
    Gas type?
    Flow rate?
    Maximum amps?
    Filler thickness?
    etc.

  12. #12

    Default

    I remember on my Lincoln tig355, an early square wave machine from late 1990s, I could set to 68% electrode negative. I was under the impression with the inverter I could nearly eliminate the etching with the capabilities of the freq and cleaning. I do think something has changed on my EX 250. It used to keep its point and provide narrow etching.

  13. #13

    Default

    I generally have a 1/8 stand off with the cup tilted about 15 degrees. I should mention I have been tig welding all since 1978, so my basics are good.

  14. #14

    Default

    Things change a good bit with an inverter though. If you can help us out with a clearer picture, that will give us something to go on.

  15. #15

    Default

    Ok. Let's see. 3/16 al sheet. 150-160 amps. 3/32 tungsten. LPH-10. Pure argon. 3/32 electrode. 4043.

  16. #16

    Default

    tungsten type? Point?

    150-160 amps can be at the top of the range for 3/32 (where you'll see more instances of splitting) depending upon the frequency and balance settings of the AC.
    I'd bump it up to 180 amps for max pedal amps...even right at 200. Minimum recommended amps for 3/16" aluminum is typically 180 amps ( 1 amp per thousandth) or slightly above. It does sound as if you may be running a little cool...thereby going too slow.

  17. #17

    Default

    Thanks Mark. I'll give that a try.

  18. #18

    Default

    Are you using pure tungsten?

  19. #19

    Default

    Absolutely not. I am variously using 2% thoriated, 2% lanthanate and ceriated.

Similar Threads

  1. AC balance cleaning 200DX ?
    By jaso1 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 10
    Last Post: 09-29-2015, 06:18 AM
  2. AC cleaning gone?
    By Infidel in forum TIG Welding (GTAW/GTAW-P)
    Replies: 16
    Last Post: 09-14-2012, 12:38 AM
  3. ac balance on stickmode
    By DannyB1954 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 25
    Last Post: 04-03-2012, 01:37 AM
  4. What is better AC amperage or AC balance?
    By srp in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-28-2012, 08:58 AM
  5. Spring Cleaning...
    By wruehl in forum Personal Projects (no welder required)
    Replies: 13
    Last Post: 04-28-2011, 11:18 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •