Share
Results 1 to 4 of 4

Thread: Power-i-Mig 250

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. #1
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default Power-i-Mig 250

    Got my Power-i-Mig 250 test it out using standard setting of the MTS250S but tried the stitch weld see what it would do.
    Setting:
    Stitch Weld - Lowest
    Spot Weld - number 2 the first weld and number 3 second the weld
    Arc Force - 6
    Volts - 22.1
    Amps - 254

    Click image for larger version. 

Name:	First test on Power i Mig 250 S-6.jpg 
Views:	538 
Size:	139.5 KB 
ID:	11449Click image for larger version. 

Name:	Second  test on Power i Mig 250 S-6.jpg 
Views:	2794 
Size:	137.8 KB 
ID:	11450
    Last edited by Kempy; 12-20-2013 at 11:27 PM. Reason: ADD
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

Similar Threads

  1. Power Pro 256 power on issue
    By wheelrdealer in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 02-27-2019, 03:47 AM
  2. Power Tig 250EX Power Cord Connections
    By Chris411968 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 01-31-2010, 07:58 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •