Share
Results 1 to 20 of 21

Thread: Amps don't reach preset while welding, is this right???

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default

    Running with the pulse, it will move around, and definitely not show max amps. Depending on the balance and the frequency settings, the readings will change because of the way the meter is calibrated. Also if the foot pedal gear has slipped on the belt, it could read less.

  2. #2

    Default

    Yea, make sure the pulse is off. That will cause the display toggle between the amp levels.

    Also you can ohm the pedal and make sure it is going all the way. 3-4 and 4-5 are the pins to check ( low to 50K and 50K to low on the two). Do you get all the power you need with the trigger?

    So glad I am not typing from my samsung tablet
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. Default

    Come On guys,,,, If I was in Pulse, I would have mentioned it

    120Hz - 30% - 1/8" electrode all the regular settings for doing new 1/4" Alum...

    BUT, my pedal IS giving me some surprising readings from 3-4-5

    I get 3-4 2Low and 35-40High (Off to Full)
    I get 4-5 55High and 20Low "

    In 3-4 I Go Full and get different readings each time, usually 35-38 Ohms but never higher than 40. Does this mean I have a problem with my pedal? I'm gonna open it up and take those reading from the Pot itself to eliminate a problem with the wire (which I have repaired from having dropped a 300Ltr cylinder on it from 8" off the cart, but maybe another conductor got damaged I didn't notice )

    But, to be clear, you're saying the digital display should read 250A while welding, Full Pedal, no-pulsing, if it's set to that?
    Last edited by Blaster; 12-14-2013 at 05:03 PM.

  4. #4
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    Yeah, or near to it.

    Sounds like either the sprocket on the pot is loose, or the pot is going south. It should be at least consistant. (ps "20Low" is in Kohms not ohms right? It's not autoranging right? And "55high" is in K ohms too right? You know, only a factor of 1000x here! )

  5. Default

    OK, so I opened the pedal and was surprised to find things looking so Out-of-Wack

    First, the Belt isn't fully running on the cogged Gear, it's 1/2 derailed because it isn't lined-up with the relief in the roller that the belt stays centered in. I can only assume it was assembled this way and not that way it's designed to be.

    Second, the Belt and Gear appear to have differing TPI (or per mm I'm sure) because the teeth engage fully in only 3-4 places then ride-up, on top of each other, on the way to the attachment point (not the spring). Whole thing looks kinda Mickey Mouse to me.....

    Just getting it open is an experience in poor design. Really,,,,, #1 Phillips (or ISO I guess) pointing down to the floor. These tiny screws are the "feet" I slide the pedal around on? THEY won't be going back! I picked the crud out of them but still had to resort to pliers to get 'em out...

    So here's what I had at the pot (I knew I could repair a wire properly ) Grey=5 / Brown=3 / Green/Yellow=4 / I assume 3 is the wiper.

    With the pedal "Floored";

    .............55
    ........... /...\
    ........../.......\
    ....Grey...Brn..Gr/Ye
    ......\......../\......./
    .......\...../...\...../
    .........35.......22


    After realigning the gear and resetting it's position;

    .............55
    ........... /...\
    ........../.......\
    ....Grey...Brn..Gr/Ye
    ......\......../\......./
    .......\...../...\...../
    .........54.......55

    The only thing is, the "at rest" readings for 3-5 I can get to 1 BUT the 3-4 is about 5 (if I adjust it lower it doesn't hold, drifts into the 100's so I assume it off the mark inside) Also I made sure the Phillips Screw "Stop" was hitting...

    Is this going to be OK, as long as I have 5-3 at 55 pedal OFF and 3-4 at 55 FLOORED?

    What's with the Belt Tooth / Gear Tooth mismatch? Is this going to continue to give me trouble?


    .

  6. #6

    Default

    Sounds like the rack and pinion (belt and gear) in the pedal skipped like Mark said. We had to mention pulse to cover other things people do miss. Did you test full power without the pedal?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. Default

    Didn't try, just opened the pedal. I haven't yet welded with it. I assume this will make a difference!

  8. #8

    Default

    Something doesn't add up in your measurements. A potentiometer of value R should always measure R between pins 1-3, and the values of pins 1-2 and 2-3 should always sum to R. With the pot fully turned one way, you should read 0 ohms between 1-2 and R between 2-3, and with the pot fully turned the other way, you should read R between 1-2 and 0 between 2-3.

    In your second diagram, you show 55 ohms between 1-3, which is consistent with the pot value that was given previously, but then you show 54 ohms between 1-2 and 55 ohms between 2-3, which would only be correct if it was a 109 ohm pot, in which case you should measure that value between pins 1-3.

  9. #9

    Default

    he is checking at the foot pedal plug not the pot inside.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. ? on welding amps/voltage
    By nickw698 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 11-17-2014, 04:51 AM
  2. New Customer...(Maybe..!!)...Looking for 300 amps
    By A-T-O-M in forum Pre-sales, Sales and Shipping questions
    Replies: 18
    Last Post: 11-02-2013, 03:15 AM
  3. Low Amps and HF
    By brianscott in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 02-12-2012, 05:45 PM
  4. 250 ex 250 amps ac
    By jdt1986 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 07-09-2011, 11:51 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •