Had to weld a Genie lift that was damaged by another lift the job site superintendent said it had to fix before it could be used. Straightened the tubes with chains and using the other lift to hook to two hour done and ready for work.
Everlast was looking for pictures live working with Everlast welders this is the closes I could get using my MTS250S and Spool Gun.