    Originally Posted by JimMinKent

    Oh boy, you just got me thinking...

    With all the timers on board the EXT, a guy should be able to spot weld, And We Can!

    For a say, 60 amp 2 second spot weld do this:

    2T mode
    AC or DC your choice,
    Pre-flow = 0.5 (my standard setting)
    Start amps = 60
    Upslope = 0
    Welding amps = 60
    Downslope = 2.0 sec
    End amps = 60

    Bingo, just let off the switch as soon as she lights off, and you've got a burn time the duration of your Downslope setting.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  2. Default

    I think this is a handy tip and it's unique to the 255 EXT, I wrote it up in my long post but it'll be easier to find here.

    I use the Pedal mode AND the 2T mode with the foot pedal. In Pedal mode, I get variable amperage control, and in 2T mode, I get a burst at the panel amps setting.

    For example, setting the panel to 200 amps, in 2T the pedal acts as the torch switch, and I get an instant 200 amp burst, great for hot tacking. Then, simply press the button to select Pedal, and it's back to normal welding without ever swapping out the pedal and torch switch connections.

    This works because the EXT doesn't use the remote pot in 2T, but rather is poised to run the sequencer parameters.
    Jim

    Everlast PowerTig 255 EXT - Bugatti Veyron
    Everlast PowerTig 250 EXT - Sent home by Ricksha
    Everlast Power I-Mig 140E - Handy little helper
    Everlast PowerArc 140 ST - Rapid Response Unit
    Miller Syncrowave 250 - Old Ironsides - Sold
    Miller Maxstar 150 STH - Nice, nice, nice
    Miller Spectrum Thunder Plasma Cutter - Cute
    HyperTherm MAX43 Plasma Cutter - Good worker
    Lincoln PowerMig 255 - Workhorse shop Mig
    ReadyWelder Spoolgun - Great portable gun

Similar Threads

  1. PowerTIG 255EXT everlast branded cover?
    By ronmartin in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 06-28-2015, 02:42 PM
  2. New 2015 PowerTIG 255EXT
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 34
    Last Post: 10-19-2014, 12:42 PM
  3. PowerTig 255EXT got CODE 805
    By Kempy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 26
    Last Post: 12-08-2013, 07:33 PM
  4. Welding Tips & Tricks Reviews the Everlast 250 EX
    By jtybt in forum TIG Welding (GTAW/GTAW-P)
    Replies: 32
    Last Post: 06-05-2013, 03:57 PM
  5. Welding Tips And Tricks Powerpro 256 Reveiw
    By Titan winch in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 10
    Last Post: 09-03-2010, 02:26 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •