    Completely spaced taking a pic.

    Here is what I meant by the swing out hinge;

    Click image for larger version. 

Name:	drop hinge.jpg 
Views:	556 
Size:	80.6 KB 
ID:	11656

    With the tailgate closed, it will be flush with the bed walls, and be 1/32"ish above the deck. When open, it will be 1/4"ish away from the bed.

    I'm sure there is a math formula to tell you where the pivot point needs to be given the thickness/depth of the tailgate to rotate 90* and be flush with the bed as shown in the pic. Layman's method will be trial and error, and easiest with a mockup.

    My boss wanted the tailgate to have a flush bed with the tailgate all the way down, and it is not strong enough to support the amount of weight these guys will put on it if it was held at 90*. I cold have made it stronger, but it would have weighed waaaaayyyy too much. We don't have the tooling to bend sheet metal to build in structural support instead of adding ribs.

    If you did not want a surface mount hinge, I'd go look at a pickup - same principle, except that under the tailgate, there will have to be a cut out area.
    Last edited by sticks; 01-04-2014 at 12:16 PM.
    Sticks
    Field Service Tech for a Concrete Paving Company
    Location: The corner of "No" and "Where"

    "If they break it, we will fix it"

    AKA

    "Find some scrap and build a new one"

Similar Threads

  1. sdr kel's fabrication work using everlast 200dx
    By sdr kel in forum On Road Fabrication
    Replies: 4
    Last Post: 02-27-2014, 07:58 AM
  2. Project 3 from agent4573 - Category - On Road Fabrication
    By agent4573 in forum On Road Fabrication
    Replies: 0
    Last Post: 01-03-2013, 01:36 AM
  3. This is project 1 from zoama585 - 8' x 12' Flatbed Trailer
    By zoama in forum Other Custom Fabrications
    Replies: 0
    Last Post: 09-09-2011, 04:34 AM
  4. project # 3 flatbed :) o i love this one but i never finished it :(
    By yotarover in forum Personal Projects (no welder required)
    Replies: 1
    Last Post: 06-03-2011, 04:57 AM
  5. Flatbed
    By yotarover in forum Other Custom Fabrications
    Replies: 1
    Last Post: 07-14-2010, 02:38 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •