Hi,
Just recently purchased a PowerPro 205S, sadly it had a little board level infant failure and its replacment is in route... It was an odd failure, I had used it a few times on DC and AC TIG and Plasma modes with no real difficulty and at the time I was trying out the pulse function, AC on an 1/8" 6061 sheet and after a few test beads at various currents and pulse settings it just stopped giving power to the arc, HF start would fire but no arc power and the overcurrent light would come on and not go off until power was cycled, then just come on again when you tried to light up..... Gas flow was fine and everything else was working but something cooked in the power output i guess..
Anyway, anyone seen anything like this before? At any rate hope this is just a fluke failure and not a weak link in the design, I wasnt really abusing it at the time..... Oh well, I hope to be able to use the unit primarly for 6061 fabrication and 440 Stainless work mainly with some 4130 tubing and mild steel framing etc. work for various projects. Artwork, and shop support functions, building tooling/fixtures for work and kinfe fabrication and what not.. So far I really like the unit in so far as its design and use, seems like if it runs and is reliable it should do everything I need... hope to report good things, soon,
Thanks!
GaRy H. Charleston, SC - RO635




Reply With Quote