Share
Results 1 to 10 of 10

Thread: Where are you getting your consumables?

  1. Default Where are you getting your consumables?

    As the title states, specifically looking for stick and tig consumables as I just got a new itig 200. Laws, inline, craigslist, etc? Thanks.

  2. #2

    Default

    To get started, I'd get the from my local welding supply store.

  3. #3

    Default

    I like http://www.weldingcity.com/ They have the best deal I've found on 2% lanthanated tungsten and torch parts.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    All of the above.

    www.river-weld.com and www.weldingcity.com for various TIG parts.
    LWS for gas, filler, stick electrodes, gloves, etc. (stuff that isn't practical to ship or want to see in person)
    Industrial hardware store for electrodes, MIG wire, tips, filler, flux, wire brushes, bits and pieces, elevator bolts.
    HomeDepot last minute weekend/late night basic electrodes, MIG wire, tips, etc.
    Autozone 24 hour MIG wire
    www.weldmonger.com TIG fingers
    ebay.com bits and bobs
    Long arc, short arc, heliarc and in-the-dark!

  5. Default

    I do shop at my LWS, and will get my gloves and gas there as well as filler to get started. I just was not sure if filler metals are cheaper online compared to LWS. Next purchase would be a pedal for this machine.

  6. #6

    Default

    The money you'd save in the purchase would likely be eaten up by the shipping.

  7. #7
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by performance View Post
    The money you'd save in the purchase would likely be eaten up by the shipping.
    There is a little truth to this...unless you're dealing with a company whose initials are A-I-R-G-A-S ! What I do is buy the minimum from the LWS so I can try the consumables, then I simply order online (from weldingcity.com, most of the time) the next time I need consumables and know exactly what I want. I buy in quantity when placing online orders so that I can justify the shipping costs, but most of the time, it's not that much. I've found that certain items (like any 309 filler) is unavailable at particular LWS, so I have to purchase it online.

    Andy
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  8. Default

    Airgas is a rip off. In the town near me there used to be 3 welding suppy companies but airgas bought them all out then raised prices to rediculous levels. I just refilled a 330 cu. ft 75/25 it cost me $115 and a 132 cu. ft. acetylene cost me over $90 from air gas. I see there is a new supplier in town now so I called them to see what there prices are, they were about 30% less than air gas. I am having them send me the application to open an account with them and when my leases are done I will stop dealing with Airgas all together.
    Last edited by TheGary; 12-04-2013 at 01:20 AM.

  9. #9
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    I predict that Airgas will suddenly decide they can operate for 30% less, as customers start defecting to the competitor. "But wait! We'll match their price!" In which case they should expect to hear "It means you've been overcharging me for the last X years I've been buying from you!"
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  10. #10

    Default

    Post 4 gets my vote.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Consumables
    By rkinken in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 03-25-2016, 01:57 PM
  2. TIG consumables
    By Rambozo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 08-19-2012, 07:11 PM
  3. New consumables
    By Titan winch in forum Everlast Announcements, Contests and Promotions
    Replies: 11
    Last Post: 01-13-2011, 12:14 AM
  4. Consumables
    By weildkorp in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 02-23-2010, 08:12 PM
  5. Consumables
    By CapnMilo in forum General Welder Questions
    Replies: 6
    Last Post: 02-10-2010, 05:47 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •