here are some of my recent work using the new 2013 model everlast 200dx.
304ss down pipe.
aluminum short ram intake
here are some of my recent work using the new 2013 model everlast 200dx.
304ss down pipe.
aluminum short ram intake
Last edited by sdr kel; 11-10-2013 at 02:34 AM.
dump tube
oil catch can
power steering reservoir
(still not done, just ordered the filler neck and filter)
Looks like you have stepped in to the pro league,,,nice work,,,wish I could do that...
Some of those lies people tell about me, are true
a few more work ive done since the last time i posted here, still workin the everlast 200dx. i recently plugged it on the 220v couple weeks ago to do an intercooler and this thing got some serious BALLS. lol the whole time i was hooked up on 110v cos i was lazy to make an extention to plug it into the dryer plug.
well heres some pics
some bluish/pur on 304 16ga ss
mild steel to ss using 309l filler
oil catch can setup
dumptube for wastegate
endtanks for intercooler
stackin some dimes
tanks welded up to the core, iirc this was at 180amps