  1. Default Is there a warm up time

    I used a guys 2012 205 welder to try it on Aluminum
    No HF, preflow off, AC on, 2T pedal
    So I checked the points they were at .060 closed them to .035 still no HF
    Points did flash on machine turn on so I held the pedal for about a minute a green led came on & about 15 secs later another green led & the points are now showing a nice blue arc
    Didn't get to weld though as the Argon bottle ran out after spending most of the day looking for loose wires researching the net for info.
    Is there a warm up time after turning on the machine ? It seems like its waiting for a capacitor to charge before a relay kicks in then again for the next relay that starts the HF.

  2. #2

    Default

    Try swapping to torch switch to confirm the pedal isn't the problem. My 225LX will HF light as soon as the fault light/diagnostics complete.
    PowerTig 225LX
    PowerCool W300
    PowerPlasma 60S
    Miller 140 MIG

  3. Default

    How long from turning on the machine is it ready to go?
    You said diagnostic cycle how long does that take ?

  4. #4
    Join Date
    Oct 2010
    Location
    Nova Scotia, Canada
    Posts
    143

    Default

    under a half a second. Something weird is going on with your machine. The torch switch check will rule out a bad switch in the pedal.
    My welder flashes it's points at starup as well. I understand that's pretty normal.
    Last edited by Paul Moir; 11-21-2013 at 04:02 AM.

  5. Default

    It does the same with the torch on 4t, It didn't want to start at all I had to switch to Plasma to Hf a few times fairly quickly then the relay kicked in,

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by dgbrit View Post
    It does the same with the torch on 4t, It didn't want to start at all I had to switch to Plasma to Hf a few times fairly quickly then the relay kicked in,
    Does the gas flow start immediately or is it delayed, too? If it starts right away you might want to play with the preflow setting as the pot may have a dirty spot in it and can often be fixed my moving the control a few times.
    Long arc, short arc, heliarc and in-the-dark!

  7. Default

    Got a new bottle of argon Hf does start after quite a long delay about a minute +
    Foot pedal strikes a ark but there is no amperage control at all I have to set the amperage on the main dial .
    Machine is on 2T, preflow at min ,Post at 5 secs ,Ac on, Hf on, freq 125, balance 30
    All other knobs at zero
    Tested pedal ohms out fine between 4-5 4-3, switch works,
    Powerpro 205

  8. #8
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Sounds like you will have to send it in for repair, unless you want to try to diagnose it further.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Hard time
    By runon in forum TIG Welding (GTAW/GTAW-P)
    Replies: 14
    Last Post: 08-26-2016, 05:28 AM
  2. First time welder from Florida
    By bigboost in forum Introduce Yourself
    Replies: 6
    Last Post: 04-16-2015, 01:00 PM
  3. Login time-out
    By NWD43 in forum Forum related Questions
    Replies: 9
    Last Post: 03-13-2014, 03:51 PM
  4. Training Time
    By Tensas in forum Introduce Yourself
    Replies: 10
    Last Post: 08-21-2013, 10:04 AM
  5. First time using gas lens...wow!
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 11
    Last Post: 09-22-2012, 01:08 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •