  1. Default Clean-Up after Jig Saw cuts

    I use a Jig Saw to make most, if not all of my cuts. I notice a little contamination at times, especially when starting and or tacking. The cuts are straight but too rough to wipe down.
    Do you guys suggest filing smooth so I can Acetone wipe or just Stainless brushing?

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Interesting idea- just so I'm clear, you use this on aluminum? If the angle aren't too great you might use a flap wheel.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    Yes my experience with grinding disc's flap wheels ect is the amount of foreign matter they leave on the material, Next to a Stainless steel brush the carbide tool is the best way i have found to clean up aluminum for welding. My cutoff saw has a Non Ferous saw blade in it and leaves a clean cut that just requires acetone.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  4. #4

    Default

    I try to use a carbide deburing tool on a die grinder if possible, if not i use a clean file to smooth things up. Jig saws and band saw blades tend to leave unwanted dirt and debri in the area where you did the saw work.
    I just repaired a rigid pipe fitting tool used to pull 2 pipes together the aluminum handle had one lug busted off and i had to use a coping saw to remove what was left. The Die grinder did a great job cleaning it up and i made a new lug from a piece of 1/4" wall aluminum tube welded it and the repair worked great.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  5. #5

    Default

    I've given some areas a shot of acetone and then hit them with a wire brush if the area is a little rough.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  6. Default

    Great idea's. Thanks!

Similar Threads

  1. Clean or shine Aluminum on the cheap
    By 5440 in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 11
    Last Post: 03-28-2013, 10:43 PM
  2. Best way to clean old aluminum for TIG
    By jtybt in forum General Welding Questions
    Replies: 39
    Last Post: 03-13-2012, 01:18 AM
  3. Clean an electrode holder?
    By posixPilot in forum Stick Welding (SMAW)
    Replies: 18
    Last Post: 02-15-2012, 01:18 AM
  4. Only cuts after post-air quits
    By trickbiker in forum Everlast Plasma Cutters (PAC)
    Replies: 5
    Last Post: 02-07-2012, 05:58 PM
  5. smooth plasma cuts
    By worntorn in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 5
    Last Post: 06-29-2010, 09:58 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •