Quote Originally Posted by Rafael View Post
I need better gloves too. After about 2 inches my hand is on fire.
Two words; TIG Finger. Sometimes I use a block of wood for a place to prop my hand. Looks pretty good for a first attempt. What is your AC balance set to? It looks like you could back that down just a little. That will narrow the frosted cleaning area some. You can wrap the cable around your arm or run it over your shoulder to take the weight off your hand, to be more steady.