Is this possible????
When switching tanks, to the one on my MIG machine over in the corner, I inadvertently rolled the knob on the flowmeter and tripled the flow and couldn't see it (I guess I was Not using the "same settings" after all

) I'm using the
Gas Saver collet from CK but, would all this extra flow have turbulated anyway? The bluing on only one side and all? The welds I was doing were in the "crotch" if the 1/4" Angle, facing me, so I had earplugs in (that 175Hz is punishing...) and didn't notice the extra gas sound.
Hasn't happened since, I've swapped back to the refilled tank now. Well see....