  1. Default Less than one year old John Deere mower repair.

    Did a repair on a John Deere the guy swears he did not hit anything. Hope pictures came out OK.

    Start removing parts.
    Click image for larger version. 

Name:	2013-09-27 11.36.47.jpg 
Views:	451 
Size:	148.1 KB 
ID:	10994

    Grind out hole. There was no rust.
    Click image for larger version. 

Name:	2013-09-27 11.36.38.jpg 
Views:	443 
Size:	146.1 KB 
ID:	10993

    Tack and square up.
    Click image for larger version. 

Name:	2013-09-27 11.52.11.jpg 
Views:	464 
Size:	153.3 KB 
ID:	10992

    Weld. You can see the tear
    in the metal. He must have hit
    something. Cash is cash no matter.
    Click image for larger version. 

Name:	2013-09-27 11.36.55.jpg 
Views:	454 
Size:	146.2 KB 
ID:	10995

    I went over tear and did the back.
    Click image for larger version. 

Name:	2013-09-27 11.55.09.jpg 
Views:	446 
Size:	147.8 KB 
ID:	10997Click image for larger version. 

Name:	2013-09-27 12.21.20.jpg 
Views:	456 
Size:	155.4 KB 
ID:	10998
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	2013-09-27 11.37.02.jpg 
Views:	509 
Size:	140.4 KB 
ID:	10996  
    Everlast IMIG-200
    Dad's TIG and plasma
    Lots of tools
    Not lots of space.

Similar Threads

  1. Mower frame repair
    By joshuab in forum Welding Repairs
    Replies: 11
    Last Post: 08-23-2013, 07:40 AM
  2. John Deere Gator Cargo Bed Lift Under $75.00
    By cbmkr in forum Other Custom Fabrications
    Replies: 8
    Last Post: 08-06-2012, 12:33 AM
  3. Acutator for John Deere Gator Cargo Bed
    By cbmkr in forum Other Custom Fabrications
    Replies: 0
    Last Post: 08-04-2012, 09:23 PM
  4. John deere Gator TX Custom Brush Guard & Winch Mount
    By cbmkr in forum Off Road Fabrication
    Replies: 0
    Last Post: 07-15-2012, 02:35 PM
  5. My first ever TIG welds. Field mower repair
    By Mikeymetal in forum Heavy Equipment and Commercial Projects
    Replies: 4
    Last Post: 06-08-2011, 09:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •