  1. #1

    Default

    A tall bead can be achieved by using smaller filler, with less amps...50 or so. It can also be achieved by using higher AC frequency, and using pulse with a wide separation of pulse peak, and pulse base amps with an 50% setting for time on, and about 1 hertz.

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Why would a tall profile be desirable? Is it a cosmetics thing?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,662

    Default

    Quote Originally Posted by DaveO View Post
    Why would a tall profile be desirable? Is it a cosmetics thing?
    Since intercooler tubing was mentioned I would guess that the reason might be hose retention.
    I would agree to go to 1/16" filler and tungsten. If you are very consistent you can use your pulser, or you can also just pulse with your foot pedal. You want to add filler while you are at high amperage, pushing as much as the puddle can take, then back off the power to let it freeze, while you move forward. Then repeat. Try not to get too much heat into the part. If it gets too hot, take a break and let things cool off.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. 250DX AC Aluminum Weld Issue
    By dmost in forum TIG Welding (GTAW/GTAW-P)
    Replies: 58
    Last Post: 11-30-2013, 08:04 PM
  2. Vertical Up Tig Weld W/185 Micro on 11 Ga Aluminum
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 10-28-2012, 05:02 PM
  3. First Attempt at an Aluminum Fillet Weld
    By blasphemy000 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 08-11-2012, 10:30 PM
  4. Oxy/Ac weld aluminum for a horse stand
    By beezfun in forum General Welding Questions
    Replies: 7
    Last Post: 08-28-2011, 09:27 PM
  5. how thin of aluminum can we weld
    By www in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 9
    Last Post: 07-21-2010, 10:06 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •