With a fixed .3 pre-flow, is that enough for a 25 foot torch?
Originally Posted by srp With a fixed .3 pre-flow, is that enough for a 25 foot torch? Yes, once you initially purge the line, the heavy argon basically stays in the hose, so a small preflow is all it takes regardless of the line length.
Long arc, short arc, heliarc and in-the-dark!