  1. Default Best tig welder for thin aluminum?

    I weld aluminum everyday on my 250ex, as long as I am welding thick aluminum to thick aluminum or thick aluminum to thin aluminum it leaves beautiful welds. I have never got it to weld thin stuff like .065 as good as I would like.

    Does anyone on here weld thin aluminum on a regular basis, if so what kind of machine do you have and can you post some pics of your work?

    I would kick the idea around about buying another machine, if it was better on the thin stuff.

    Here is a pic of what I weld.

    http://i854.photobucket.com/albums/a...st250EX004.jpg

  2. #2

    Default

    I don;t think it is a problem with machine selection, rather technique or settings.

    What problems are you having?
    What machine settings?
    What filler wire size?
    What type of joint?
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    My 200Dx does a great job on .025 aircraft aluminum, Welding panels up and adding brackets to sheet parts.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  4. #4

    Default

    Quote Originally Posted by srp View Post
    I weld aluminum everyday on my 250ex, as long as I am welding thick aluminum to thick aluminum or thick aluminum to thin aluminum it leaves beautiful welds. I have never got it to weld thin stuff like .065 as good as I would like.

    Does anyone on here weld thin aluminum on a regular basis, if so what kind of machine do you have and can you post some pics of your work?

    I would kick the idea around about buying another machine, if it was better on the thin stuff.

    Here is a pic of what I weld.

    http://i854.photobucket.com/albums/a...st250EX004.jpg
    .065 isn't all that thin. Now, .0065...well that should be the machine's limit or there about. From the looks of the larger welds, it looks like you are getting way too much cleaning. I'd start there. What's your balance setting running on average? Frequency? What type tungsten? Diameter? Amps? Like to help if we can.

    What exactly is happening when you are trying to weld that thin?
    Last edited by performance; 10-02-2013 at 03:31 PM.

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Photos of the problems would help a lot more than photos of what works good.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    Quote Originally Posted by cbmkr View Post
    My 200Dx does a great job on .025 aircraft aluminum, Welding panels up and adding brackets to sheet parts.
    Wow. that's pretty thin.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  7. Default

    I spent most of the day adjusting the welder out for thin aluminum, I always use 5356 because it welds so much better on the 250ex and the Syncrowave 250. And also that is the correct filler for that alloy, on thin stuff I always drop down on tungsten size to .040.

    I was thinking kinda like Mark, needing less cleaning action but that was not what it needed. I was welding at 10% to 20% ac balance and having absolutely no luck, the arc was acting more like a cutting action. I had tried the frequency everywhere as well.

    After scratching my head for about four hours I bumped up the cleaning action to 30% and had the frequency at 250, the little 250ex then laid down some of the prettiest welds I have ever seen on .065 aluminum, I just kept going in the wrong direction with cleaning action. I still don't understand why it needs cleaning action 1/4 inch wide but that's what it took.

    So I think I answered my own question on what is the best tig for thin aluminum. EVERLAST? LOL

    Thanks to everyone that replied with help!

Similar Threads

  1. Help welding thin Aluminum PowerTig 250EX
    By joshtodd1984 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 38
    Last Post: 04-12-2016, 02:57 PM
  2. stick welder aluminum
    By jimmy in forum General Welder Questions
    Replies: 6
    Last Post: 05-25-2013, 05:45 AM
  3. TIG welder or MIG Spool Gun for Aluminum
    By Odyknuck in forum General Welding Questions
    Replies: 24
    Last Post: 12-15-2012, 03:47 PM
  4. Need a tig welder for the thin stuff
    By voss955 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 04-18-2012, 01:57 PM
  5. how thin of aluminum can we weld
    By www in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)