Share
Results 1 to 8 of 8

Thread: Cnc cutting with everlast 60s

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Cnc cutting with everlast 60s

    Hey does anybody have or know where I can get some good cutting parameters for the unit? The manual that it came with is all in Chinese...

  2. #2

    Default

    I believe this is the current manual. http://www.everlastgenerators.com/do...rplasmapdf.pdf
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    This manual covers your unit- it's from the Everlast site.
    http://www.everlastgenerators.com/do...sma%202013.pdf

    What are you working on?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  4. Default

    Does anyone have a chart as to what amperage for certain thicknesses .... Etc. ?

  5. #5

    Default

    Quote Originally Posted by FeddFab View Post
    Does anyone have a chart as to what amperage for certain thicknesses .... Etc. ?
    Faster cut = smoother cut. More amps = faster cut. You want the torch moving as fast as possible without skipping. 60amps
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6

    Default

    The manual I posted earlier was for the 60c... DaveO had the right one for the S.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  7. #7

    Default

    I generally recommend 20 amps for the first 1/8" and then 10 amps for every 1/8" after that.

  8. Default

    Quote Originally Posted by FeddFab View Post
    Hey does anybody have or know where I can get some good cutting parameters for the unit? The manual that it came with is all in Chinese...
    Your best bet will be to get the thermal dynamics 40amp unsheilded cut speed chart. These import machines dont have any kind of cut speed parameters in their manuals..

Similar Threads

  1. 256 cutting in and out mid bead
    By tnc110 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-15-2013, 01:09 AM
  2. Cutting with no eye protection...
    By CGCINC in forum Everlast Plasma Cutters (PAC)
    Replies: 23
    Last Post: 08-10-2012, 04:42 PM
  3. Anybody cutting 1"?
    By Jake98 in forum Everlast Plasma Cutters (PAC)
    Replies: 19
    Last Post: 05-11-2012, 06:19 PM
  4. DIY dryer for plasma cutting and TIG welding. Dross cutting or TIG electrode fur
    By everlastsupport in forum Welding articles from Professionals (knowledge database)
    Replies: 0
    Last Post: 03-15-2012, 01:08 PM
  5. cutting at an angle
    By McClary in forum Everlast Plasma Cutters (PAC)
    Replies: 4
    Last Post: 12-29-2011, 01:01 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •