    So I started playing with my tig the other day. I got to use it for about 20 minutes until I noticed a puddle of liquid on the floor. One of my hoses had a hole in it. When we pulled the sleeving we found that it was the power hose and it looked melted. Am I correct in thinking that the power hose on a tig carries liquid? I'm using a wp-20 torch. Maybe I let it cross the ground cable somehow and it arced through? I'm new to tig so it kind of surprised me.
    Owner/Operator of Breakneckmoto
    Used motorcycles and parts

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by breakneckmot View Post
    So I started playing with my tig the other day. I got to use it for about 20 minutes until I noticed a puddle of liquid on the floor. One of my hoses had a hole in it. When we pulled the sleeving we found that it was the power hose and it looked melted. Am I correct in thinking that the power hose on a tig carries liquid? I'm using a wp-20 torch. Maybe I let it cross the ground cable somehow and it arced through? I'm new to tig so it kind of surprised me.
    Yes, the power hose carries the return coolant. This cools off the power cable and is the first thing to die upon coolant failure. The most common way that happens is by running the torch without coolant. It doesn't take long at all, either. Or by outside damage from hot or sharp metal. Which is why you usually use a hose cover. The cable is usually replaceable. What brand torch are you using?
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Quote Originally Posted by Rambozo View Post
    Yes, the power hose carries the return coolant. This cools off the power cable and is the first thing to die upon coolant failure. The most common way that happens is by running the torch without coolant. It doesn't take long at all, either. Or by outside damage from hot or sharp metal. Which is why you usually use a hose cover. The cable is usually replaceable. What brand torch are you using?
    Pretty sure it's a weldcraft torch. I hadn't taken the sleeve off and inspected the cables, so it could have been there when I got the machine. It didn't leak immediately, it started after maybe 15 minutes of run-time. The cooler had plenty of fluid so it didn't run dry and was pumping out when I saw it. I already ordered a replacement cable/hose for it.
    Owner/Operator of Breakneckmoto
    Used motorcycles and parts

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Might be a good time to flush and change coolant. You might have some crud in there that blocked the flow for a bit. Especially if it has been sitting around for a while. Blow out the torch while you have it apart, too. The passages are pretty small so things need to stay clean.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5

    Default

    Quote Originally Posted by Rambozo View Post
    Might be a good time to flush and change coolant. You might have some crud in there that blocked the flow for a bit. Especially if it has been sitting around for a while. Blow out the torch while you have it apart, too. The passages are pretty small so things need to stay clean.
    Will do, I was planning to change the fluid anyways. Is there any specific kind of fluid I should be using? (Bernard cooler) The guy I got it from had an empty bottle of Miller coolant sitting on it when I bought the machine.
    Owner/Operator of Breakneckmoto
    Used motorcycles and parts

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by breakneckmot View Post
    Will do, I was planning to change the fluid anyways. Is there any specific kind of fluid I should be using? (Bernard cooler) The guy I got it from had an empty bottle of Miller coolant sitting on it when I bought the machine.
    Any good brand of TIG coolant will work fine. Use distilled water if it is a concentrate that requires dilution. There is usually a screen filter on Bernards that you should clean out, too. It's under the big acorn nut on the pump.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I use antifreeze for swimming pools it is made for pumps and plastic parts and rubber parts you will have to use distilled water to get the right amount of antifreeze for the weather you are in. As DaveO said not to use automotive antifreeze. Most of the welding ones are set for about 15 deg. F. Good look on getting things right.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  8. Default

    That RV stuff has alcohol (or something...) in it though. I read the red, Walmart stuff, and it's says "Flammable". THAT can't be a good idea

    I think the next, best, alternative is DexCool, diluted with distilled water, and also available at Walmart...

Similar Threads

  1. Stupid question here
    By Elantramax1 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 8
    Last Post: 09-04-2014, 03:59 AM
  2. Simple Question from Newbie
    By tdkask in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 09-21-2013, 07:41 PM
  3. Newbie Question - Downside to Gas Lens?
    By greygizmo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 43
    Last Post: 01-06-2013, 05:24 PM
  4. Newbie question
    By DaveO in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 03-14-2011, 08:02 PM
  5. Newbie 225LX pedal control question
    By robsthomson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 02-17-2010, 01:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •