Share
Page 1 of 2 12 LastLast
Results 1 to 20 of 21

Thread: But welding sheet metal

  1. #1

    Default But welding sheet metal

    I've been working on a sheetmetal project where I'm making my hood into a cowl hood. This means I have to add some thin strips of metal to the existing hood. I cut and sanded the first part so it had zero gap when I butted it up to the edge of the hood. Then I started tacking it with the tig. By the third tack the metal started pull so badly that it overlapped. Next piece I put in I will add some shim stock spacers about 10thousands thick then the tacks should pull it tight. Anybody else experience this?
    My Stuff:
    Everlast PP256
    Century Mig 135
    BladeRunner Inverted Jig Saw
    HF 14" Chop Saw
    Box full of HF 4" Angle Grinders
    Home made tank roller!

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Yes, with any metal, but more pronounced with sheet metal, heating and metal shrinkage is something you have to work with as you fit pieces. It takes practice and skill to pull it off. I can't say I'm that good at it, but those that do autobody sure need to be. Generally you have two pieces that have a thin pie gap that closes up as the two parts are tacked together. There are different techniques to control shrinkage during welding. Some take shrinkage into account when making the parts, others go for the death by a million tacks and try to hold everything in place before welding. Skip stitch and or back step welding can help, too. Careful shrinking and stretching after the weld can take care of minor distortions. You can find all kinda of hot rod pros on YouTube that do crazy sheet metal manipulations, and all without any body filler!
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    When I am welding in sheet metal I try to fit the piece close to where it is going to go and then just work it into place with a body hammer as I tack around the edge. Once I get tacks all around the piece, I will place a couple tacks together and just move around the piece trying to control the heat to avoid warping it.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  4. Default

    Quote Originally Posted by Rambozo View Post
    ?... You can find all kinda of hot rod pros on YouTube that do crazy sheet metal manipulations, and all without any body filler!
    Those guys are the real master-crafters. I remember being horribly disappointed years ago when a certain custom bike show came on TV. A lot of the metal work was roughly mig'd together and the paint & body guys did all of the beauty work with filler and lots of sanding.

  5. #5

    Default

    I'm getting pretty good with the body dolly wet but I may need to buy a metal shrinking hammer/dolly. Finished welding the first seam of 6 pieces today. I'm going to grind it smooth, do some dolly work and see how much better I need to be on the next seam.
    My Stuff:
    Everlast PP256
    Century Mig 135
    BladeRunner Inverted Jig Saw
    HF 14" Chop Saw
    Box full of HF 4" Angle Grinders
    Home made tank roller!

  6. #6
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    I am getting better at tig welding sheet metal, but I have had a bit of practice from welding sheet metal in my trade for starters. The bigger sections of thin sheet are what I have trouble with still. I really get a kick out of watching my dad gas weld sheet metal when doing rust repairs on cars. Of course he's been doing it since the 1960's, and is more comfortable gas welding and using the torch to shrink metal than welding with any other process, since it comes more natural for him. MIG was just something that he had to learn for his trade in later years in order to keep up with technology, and he's good at it, but still better with oxy/acetylene. I think he will do good once I teach him the basics of tig welding. His main issue now is poor eyesight.

    In the sheet metal trade I got used to welding and metal finishing everything nicely since it's usually exposed stainless (indoors), galvanized (outdoors/rooftops), or copper (outdoors). Especially the food service type items. No bondo allowed (haha). I always make sure to put the smallest tacks possible (get in and get out ASAP to minimize heat input), use as many vise grip clamps as I can (or use cleco's), and use a backing of some nature (usually copper) when possible. Fit up is everything. And of course, the tungsten needs to be sharp, and the filler rod needs to be small (diameter). The end result is what's important, and everyone does things a little different. You just have to figure out what works for you.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  7. #7

    Default

    Put in my second piece today. Left a small gap and let the weld close it. It worked much better. I also put a lot more tacks and use compressed air to cool the panel after every 1/2" of weld. This project is going to take a lot longer than I thought!
    My Stuff:
    Everlast PP256
    Century Mig 135
    BladeRunner Inverted Jig Saw
    HF 14" Chop Saw
    Box full of HF 4" Angle Grinders
    Home made tank roller!

  8. Default

    Sounds like you've devised a solution. Please post some pictures of the work if you can!

  9. #9

    Default

    Quote Originally Posted by Ron66 View Post
    Put in my second piece today. Left a small gap and let the weld close it. It worked much better. I also put a lot more tacks and use compressed air to cool the panel after every 1/2" of weld. This project is going to take a lot longer than I thought!
    I forgot to mention, I usually leave at least a 1/16 gap around the edges. Moving around the piece if large enough will allow you to keep working without putting too much heat into one area causing warpage.



    @youngnstudly
    I thought all stainless or anything for that matter had to be back purged in the food industry for compliance.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  10. #10
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by Jason View Post
    @youngnstudly
    I thought all stainless or anything for that matter had to be back purged in the food industry for compliance.
    Sorry for the confusion, I didn't mention anything about stainless in particular since I figured Ron66 wasn't building a cowl hood from stainless that he planned to eat off of. Plus I was speaking more of the metal finishing with the stainless. You are correct though, for the most part. However, you'd be surprised how many smaller HVAC shops in my trade don't back purge when welding stainless material for the food industry. Especially when doing quick repairs on already built items, or small jobs that the tight-wad restaurant owner wants the shop to build fast and cheap. If they think they can get away with not doing it, they'll try to. Yet another reason to eat at home!
    Last edited by youngnstudly; 09-09-2013 at 10:04 AM.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  11. #11

    Default

    Click image for larger version. 

Name:	49-199.jpg 
Views:	649 
Size:	6.3 KB 
ID:	10765
    I found that these work pretty good. They leave just a small gap.
    I got mine at Harbor Freight.

  12. #12

    Default

    Some pics of my progress
    Click image for larger version. 

Name:	20130908_170002.jpg 
Views:	621 
Size:	37.1 KB 
ID:	10766
    Click image for larger version. 

Name:	20130908_140755.jpg 
Views:	643 
Size:	32.2 KB 
ID:	10767
    My Stuff:
    Everlast PP256
    Century Mig 135
    BladeRunner Inverted Jig Saw
    HF 14" Chop Saw
    Box full of HF 4" Angle Grinders
    Home made tank roller!

  13. #13
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I got the same at Princess Auto the same as in Harbor Freight in Canada we have Princess Auto and the USA have Harbor Freight.
    Click image for larger version. 

Name:	PA1.jpg 
Views:	601 
Size:	129.6 KB 
ID:	10768Click image for larger version. 

Name:	PA2.jpg 
Views:	577 
Size:	131.8 KB 
ID:	10769
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  14. #14

    Default

    Quote Originally Posted by Gman View Post
    Click image for larger version. 

Name:	49-199.jpg 
Views:	649 
Size:	6.3 KB 
ID:	10765
    I found that these work pretty good. They leave just a small gap.
    I got mine at Harbor Freight.

    I have seen those on eastwood andhave wondered if they make things easier. Usually I just fit the piece and then use my triangle magnets to hold the piece while I tack it in place. Next time I am HF I might have to pick some of these up if they are not too expensive.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  15. #15
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by Jason View Post
    I have seen those on eastwood andhave wondered if they make things easier. Usually I just fit the piece and then use my triangle magnets to hold the piece while I tack it in place. Next time I am HF I might have to pick some of these up if they are not too expensive.
    Magnets work but with Tig they do cause problems but still looking for aluminum Magnets but no luck have to use the sheet metal clamps or vice grips.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  16. #16
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    Quote Originally Posted by Jason View Post
    I have seen those on eastwood andhave wondered if they make things easier. Usually I just fit the piece and then use my triangle magnets to hold the piece while I tack it in place. Next time I am HF I might have to pick some of these up if they are not too expensive.
    I use my triangle magnets for tacking up too. I do have the issues that Kempy mentioned sometimes with them, but there's no other way around it in certain situations. It's darn near impossible to tack something up that has a gap of any nature, while trying to use one hand to hold the part in place (say with pliers). And if you can't get to the backside of the part you're welding, vise grips are rendered useless. Cleco's can be used successfully in particular instances.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  17. #17

    Default

    I guess I have never run into the issue with the magnets and TIG. I so also have clamps that I use some times and the magnets do not work for aluminum so I either clamp that or find some way to hold it whether its proping something against it or trying to hold it by other means while I tack it.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  18. #18

    Default

    Quote Originally Posted by Kempy View Post
    Magnets work but with Tig they do cause problems but still looking for aluminum Magnets but no luck have to use the sheet metal clamps or vice grips.
    Will have to google that. Alumimum magnets??

    Also, the magnets can cause problems with MIG as well. They gets us on occasion but rare.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  19. #19

    Default

    What are these problems you guys speak of? I have never noticed any problems using them.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  20. #20
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Jason View Post
    What are these problems you guys speak of? I have never noticed any problems using them.
    A strong magnet can and will attract the actual arc. So often the arc will wader away from where you are trying to point it. Similar to how a static electric charge can bend a stream of water.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Cutting Expanded Sheet Metal
    By xtreme cartz in forum Everlast Plasma Cutters (PAC)
    Replies: 55
    Last Post: 02-14-2013, 02:16 PM
  2. Strengthening sheet metal without a bead roller?
    By CGCINC in forum General Welding Questions
    Replies: 11
    Last Post: 08-09-2012, 02:39 AM
  3. What is your prefered method to cleaining metal before tig welding
    By turbo_bully in forum General Welding Questions
    Replies: 5
    Last Post: 08-24-2011, 12:20 AM
  4. Need some tips on welding sheet metal to 3/8 plate
    By Haywire in forum Stick Welding (SMAW)
    Replies: 13
    Last Post: 06-07-2011, 03:56 AM
  5. Welding on Galvanized metal
    By performance in forum Welding articles from Professionals (knowledge database)
    Replies: 5
    Last Post: 04-04-2011, 08:32 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •