  1. #21
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by Rambozo View Post
    Looks great. Thanks for the demonstration. The helium seems to make all the difference. Looks like another gas I should keep around. I haven't used it since school, and then the price was a lot more reasonable.
    The only thing with helium is it will leave the weld black on top but comes off easily water and a wire brush or soap and water. I will be cleaner if you us 25% helium 75% argon or 50/50 an a lot of heat and thicker metal.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  2. #22

    Default

    The reason the black soot is left is because the Helium is virtually leaving the weld area right after it is applied. That's the down side to helium, no one talks about. It's lighter than air, and as soon as it exits the gun, starts to float up and off. Argon is heavier than air, and stays where it is put when it is done down hand. The black is oxidation actually.

  3. #23

    Default

    Quote Originally Posted by Kempy View Post
    Zoama585
    You got the 250P how do find the pulse work on it? I is you don't have a spool gun but with it I find it so handy with the 25 ft. line the only thing you have to watch out for is tipping the gun to sharp and the gas line will kink a little and slow the flow down if you put it over your shoulder it works fine.
    I've only used pulse to weld a flowmaster muffler back together after I opened one side with the plasma cutter. I have no formal training in welding and I don't fully understand how to use the pulse feature... but I will learn.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #24
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Quote Originally Posted by performance View Post
    The reason the black soot is left is because the Helium is virtually leaving the weld area right after it is applied. That's the down side to helium, no one talks about. It's lighter than air, and as soon as it exits the gun, starts to float up and off. Argon is heavier than air, and stays where it is put when it is done down hand. The black is oxidation actually.

    I modified a nozzle to get the flow on the weld better, it did help the black. I made no changes to the settings just the nozzle would have to do more test to get the weld better. Maybe I will try welding upside down and let the helium work the way it wants.
    The argon does make a nice weld and cleaner. It only took a few swipes with a wire brush and it was clean.
    Click image for larger version. 

Name:	1 org. nozzle.jpg 
Views:	351 
Size:	133.1 KB 
ID:	10725Click image for larger version. 

Name:	2  new nozzle.jpg 
Views:	339 
Size:	135.2 KB 
ID:	10726Click image for larger version. 

Name:	3 test with new nozzle.jpg 
Views:	354 
Size:	136.3 KB 
ID:	10727Click image for larger version. 

Name:	4 clean .jpg 
Views:	358 
Size:	124.7 KB 
ID:	10728
    Last edited by Kempy; 09-03-2013 at 02:32 PM.
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

Similar Threads

  1. Cast Iron Car block tig welded
    By Kempy in forum Welding Repairs
    Replies: 18
    Last Post: 06-20-2023, 10:22 AM
  2. question on welding cast iron
    By revkev6 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 02-26-2017, 02:18 PM
  3. Cast Iron
    By Estarial in forum General Welding Questions
    Replies: 13
    Last Post: 07-15-2011, 05:36 PM
  4. bandsaw repair, cast iron
    By starvingartist in forum Welding Repairs
    Replies: 1
    Last Post: 06-24-2011, 02:29 PM
  5. weldig on cast iron
    By yotarover in forum General Welder Questions
    Replies: 4
    Last Post: 03-06-2011, 09:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •