  1. Default Recent Project (250EX) - Welding Cart from Hell

    Thought I'd share this... I've wanted a nice mobile setup for a while, and finally went for it. Used aluminum scrap (truck drive-shafts, snow-rakes, posts, misc tubing), modified a 700-lb dolly with some large wheel-chocks, bolted on some locking swivel wheels and made two wooden platforms. It holds my argon cylinder (any size), 250EX, three-drawer tool cabinet, bench grinder, vice, and large misc bin underneath.

    Then I realized my colossal mistake...
    It's not green!! (I kinda just rolled with the original dolly color).







    Added an abs plate for the foot of the dolly, and a heavy plastic-coated chain to secure the cylinder. Best thing is, the whole thing rolls into the back of my van.

  2. Default

    That looks huge! You have to post some pictures of it loaded.

  3. #3
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Quote Originally Posted by Gandalf View Post
    It holds my argon cylinder (any size), 250EX, three-drawer tool cabinet, bench grinder, vice, and large misc bin underneath.
    That is a beast, for sure, but it looks like you've got "cylinder containment" covered for sure. I just hope the ramp from the van isn't too steep!
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  4. #4
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    What a great use of scraps! I never would have thought to include a hand truck into the picture but it is obviously up to it's task of holding your cylinder in place, regardless of the size you choose! I agree about you taking a picture with the cart loaded...I bet that green welder will look nice in contrast to your welding cart's blue finish. Do you plan on sealing or painting the wood, or leaving it bare?
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Looks interesting. It's fun to try and figure out where all the re-purposed items are. I'm also curious to see it loaded up. I am concerned about the clearance under the hand truck portion. Looks pretty tight and that is with no weight. At least with the pneumatic tires you can raise it a little with additional pressure.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    That looks really neat. Are you planning on keeping all of your supplies on it? It looks pretty big for just the welder/cooler.
    Owner/Operator of Breakneckmoto
    Used motorcycles and parts

  7. #7

    Default

    my only concern with the design is the clearance of the plate that will hold your bottle,,,looks like it could be an inch or two higher..which in it self is a major mod...as hand carts are made to sit on that plate...
    Some of those lies people tell about me, are true

  8. Default

    Quote Originally Posted by breakneckmot View Post
    That looks really neat. Are you planning on keeping all of your supplies on it? It looks pretty big for just the welder/cooler.
    Yes, it's meant for pretty much everything, plus has room for the cooler below (don't have a cooler yet).

Similar Threads

  1. Welding Cart For 250EX And PP60 Plasma Cutter+ Boat Project
    By zoama in forum Other Custom Fabrications
    Replies: 19
    Last Post: 01-29-2016, 02:55 AM
  2. First Project: Welding Cart
    By Glassbeaver in forum Other Custom Fabrications
    Replies: 6
    Last Post: 06-19-2014, 03:51 AM
  3. NOt welding related but some of my recent hat work
    By ironmanjay in forum Other Custom Fabrications
    Replies: 10
    Last Post: 06-07-2013, 10:34 AM
  4. 250EX-Aluminum welding cart
    By 5440 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 03-25-2013, 10:18 AM
  5. First Welding Project - You guessed it... a welding cart
    By EmptyNester in forum Hobyist Projects
    Replies: 19
    Last Post: 10-12-2011, 03:30 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •