    I have this 30 lb roll of .045" MIG wire. I presume it's a SS wire but the label is very faded.

    I'm more or less guessing on these numbers but this what I think I can read.


    TYPE: ER38

    Size: .045"

    W.O. #: 95A075

    Specs: AWS A5.9

    Again, I'm just guessing. Some of the numbers may be letters or some of the letters may be numbers...and some of the numbers may not be all there.

    There is a label saying it contains Chromium and nickel and is known to be carcenogenic.

    Thanks.


    OH! I wanna use it fir TIGing SS. It puts down a nice small bead all shiny.
    Last edited by jtybt; 03-08-2010 at 05:58 AM.
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

  2. #2

    Default

    It probably says ER 308 or 308L. I believe that using it for Tig should be fine, as it is basically very similar to cut lengths of Tig wire, just smaller.

  3. #3
    Join Date
    Oct 2009
    Location
    Too far North! Midwest USA
    Posts
    59

    Default

    Being the wire is .045 its the same as what I use but to use it where you need a larger diameter I take about a 4 foot piece and fold it in halve and put the loose ends next one another in a vice and the the loop end in a hook or eye bolt in your battery drill and pull hard and run the drill and twist it tight. It will work well as a larger wire. Tried 2 pieces together but couldn't get a uniform twist. If you didn't twist tight enough just fuse the end together then it won't fray.
    dwdw

  4. Default

    Thanks guys. I guess it forces me to keep my temps down because it's thin. For the most part, I'll be welding 1/16" (.063") wall SS tubing with maybe 1/8" bases or gussets so it looks like it'll work out for me. Most of the stuff will be 304 or 316 though I have stuff that's tuffer'n sh*t to grind. I hope it'll be OK.


    I'm embarrassed to say I've been using it for making crab pots(traps)
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

Similar Threads

  1. MIG wire cleaner
    By Schuh in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 6
    Last Post: 06-11-2013, 04:40 AM
  2. MIG wire cleaner
    By Schuh in forum Technical Bulletins and Tips
    Replies: 1
    Last Post: 06-09-2013, 12:44 AM
  3. Who Makes The Best Mig Wire ?
    By zoama in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 45
    Last Post: 07-31-2012, 12:01 PM
  4. How do I wire up a P80 for CNC use ?
    By someguy in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 07-28-2012, 01:14 PM
  5. Replies: 26
    Last Post: 02-22-2012, 11:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •