 Originally Posted by 
Depdog
					
				 
				All this pot talk makes me want to cook or smoke!
So if I'm reading you correctly, the new 185 can use a 25k ohm pot and it should work correctly?
CK makes a fingertip control for Hobart that is 25k ohms.
			
		 
	 
 Put the Everlast 7 pin plug connector onto my old Hobart CK linear amp controller that had a old military 10 pin connector and a 25K pot, put it on my 255EXT it works but it is at full power just over 1/2 way. The 10K linear amp from CK give me full power just over 3/4 travel mark. The  Everlast Amptrol with a 47K pot gives me the complete range of the pot as it hits the end it was at full power 250A.
 The 250EX with the 25K controller it gave me full range but 8 to 245A and with the 47K Amptrol full range 6 to 250A now with with the 10K CK it gave me 6 to 230A. 
That's it no more potentiometer to test.
 I could test them all on the MTS250S some day.
				
			 
			
		 
			
				
			
			
				Everlast PowerTig 325EXT (Canada)
Everlast Power I Mig 250 (Canada)
Everlast PowerPlasma 80S (Canada)
Everlast PowerCool W300 (Canada)
Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
Miller Dynasty 400 wireless(Canada)
Millermatic 252 plus 30A Spoolgun(Canada)