Plenty of variation from brand to brand in taking up moisture too. I had a cardboard box of Lincoln from Home Depot that lasted for many years, next batch was Hobart and I left a half a stick hanging in the stinger overnight and by morning it was soggy. Also makes a big difference whether you live in Florida or Nevada.