Originally Posted by
travis
ok I used some 3/32 6011 and really went though the rods pretty fast iam thinking 1/8 inch would work better iam welding some 3/8 to 1/4 inch steel and iam thinking of trying some 7018 seen some youtube vids and it looks like nice beads any input would be nice .......oh I have the powerultra 205p ...thanks
On that thickness 3/8 to 1/4 ,, 1/8 6011 would be a better choice than 3/32,,,7018 1/8 can work very well although it require more amps for the rod size over 6011,,, my point is,, go with what you are good at,,,,trying a new type of rod is always interesting,,,it has it's draw backs,,,in the case of 7018 ,,down hill welding is not reccomended..
Some of those lies people tell about me, are true