Gary,
Disagree on the 6011. If you have DC, 6011 still runs better than 6010. No reason to run 6010 unless a specification calls for it. It's not an AC only rod. It's both, and always has been.
6013 is often classified as medium penetration. It's a great fab rod, and great for GP welding.
7024 will run horizontal.
7018 is often required now for root pass welds, and many places have been replacing 6010 now for insurance reasons.