  1. Default Powertig 225 LX display erratic in pulse mode

    Hi I've had my 225 LX for about a month and a half and I've just gotten around to trying the pulse mode. When I turn the pulse switch on the display starts displaying a series of random numbers and I can't tell what my amps are set at. I thought maybe it was showing me all of the pulse setting one after the other but the numbers keep changing randomly so that doesn't seem like what it is doing. Has anyone else had this issue? Any help would be appreciated. I'm wilding steel and am in DCEN if that helps. Thanks
    Aaron

  2. #2

    Default

    Quote Originally Posted by Aaron View Post
    Hi I've had my 225 LX for about a month and a half and I've just gotten around to trying the pulse mode. When I turn the pulse switch on the display starts displaying a series of random numbers and I can't tell what my amps are set at. I thought maybe it was showing me all of the pulse setting one after the other but the numbers keep changing randomly so that doesn't seem like what it is doing. Has anyone else had this issue? Any help would be appreciated. I'm wilding steel and am in DCEN if that helps. Thanks
    Aaron
    Aaron,
    We have several threads dedicated to this question as they are repeated regularly...and it's also in the new manuals. Do you have a new style? I wasn't aware they were out. It's almost the same as the 250EX now...if there isn't a new 225 manual up, use that one and just minus the start and end amps and top end pulse frequency...everything else is similar.

    But to repeat it again:

    There's no way to make the unit cycle 250 times per second if the pulse frequency is 250 and have it reflect in the display. What you see is perfectly normal. The display "samples" the output of the pulse at a different frequency of the pulse, so it may sample the pulse while its rising, falling or even at the bottom of the top. It's not random, but to your mind it may appear that way. There's no way to make those sync up. If the display cycled 250 times per second, you wouldn't see anything but 888 likely. When setting the pulse after it is first turned on, you have several seconds in which to set the pulse before the display starts cycling. If you go beyond that default time, you have two choices. 1) Turn it off and then back on to finish setting, 2) Turn pulse frequency to a minimum and the display will cycle slowly enough to register. For me, I just set pulse to a minimum to start with and adjust pulse frequency last.

  3. Default Thanks

    Quote Originally Posted by performance View Post
    Aaron,
    We have several threads dedicated to this question as they are repeated regularly...and it's also in the new manuals. Do you have a new style? I wasn't aware they were out. It's almost the same as the 250EX now...if there isn't a new 225 manual up, use that one and just minus the start and end amps and top end pulse frequency...everything else is similar.

    But to repeat it again:

    There's no way to make the unit cycle 250 times per second if the pulse frequency is 250 and have it reflect in the display. What you see is perfectly normal. The display "samples" the output of the pulse at a different frequency of the pulse, so it may sample the pulse while its rising, falling or even at the bottom of the top. It's not random, but to your mind it may appear that way. There's no way to make those sync up. If the display cycled 250 times per second, you wouldn't see anything but 888 likely. When setting the pulse after it is first turned on, you have several seconds in which to set the pulse before the display starts cycling. If you go beyond that default time, you have two choices. 1) Turn it off and then back on to finish setting, 2) Turn pulse frequency to a minimum and the display will cycle slowly enough to register. For me, I just set pulse to a minimum to start with and adjust pulse frequency last.
    Thanks for the reply Mark,
    Sorry about the reposting of a familiar thread, I did try to search the forum for this problem but came up empty. I guess I haven't got the swing of how to use the search engine effectively yet. It's good to know that this is not a malfunction of the display. The pulse function has been working fine and is a great help in welding this steel mesh without blowing it out. I don't think I have a 'new style', mine is an analog model. I looked at the manual but it did not give any information about how the display functioned in pulse mode. The manual is for several of the models including the 250 EX. Anyway I'm happy with the welder and slowly getting my feet wet with its different functions. Thanks again.
    Aaron

  4. #4

    Default

    No, the new units are analog as well. But do you have the new case design? A new 225lx SHOULD look like this if it is from the new shipment. And the link to the new 250ex manual is here on our website:
    http://www.everlastgenerators.com/do...werTIG-NEW.pdf

    And the page that information is on is: page 22, section 4.1
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	PowerTIG 225 LX.jpg 
Views:	329 
Size:	118.7 KB 
ID:	10416  

  5. Default

    Mine is the older model without the plastic cover on the front. Thanks for the link to the new manual, it seems to have a lot more information.
    Aaron

  6. #6

    Default

    Did you buy it used or as a refurb? That model hasn't been around since 2009. Didn't you say you just got it?

Similar Threads

  1. Powertig 185 display functions?
    By DaveBonds in forum General Welder Questions
    Replies: 2
    Last Post: 03-23-2014, 07:17 PM
  2. 2013 Powertig 200DX 200 Amp 110/220 Dual Voltage Pulse AC/DC
    By magichat in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 09-23-2013, 06:22 PM
  3. PowerTIG DX200 DC works awesome! A/C mode blew up my Gas-lens!
    By spoolxexo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 06-01-2012, 02:03 AM
  4. Erratic start with foot pedal
    By jtybt in forum TIG Welding (GTAW/GTAW-P)
    Replies: 27
    Last Post: 08-03-2011, 06:40 PM
  5. Question re: operation of pulse mode on PowerTig 200DX
    By Tantalum711 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 07-08-2011, 11:21 PM

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •