  1. Default mig wire for tig welding steel

    i have some mig wire (lincoln super arc l 56) can i use it as filler for tig welding steel?

  2. #2

    Default

    Yes. If you are making an open butt weld, just remember to keep your gap tight and your amps low. For fillet welds, just keep in mind that you will be feeding a lot wire because of the diameter of the wire you are using.

  3. #3

    Default

    Generally, yes, it shouldn't be a problem, especially if the TIG wire has an equivalent number assigned to it.

  4. Default

    how much cfh of argon do you reccomend?

  5. #5

    Default Argon

    Quote Originally Posted by steve1989 View Post
    how much cfh of argon do you reccomend?
    I would think that 15 to 20

  6. #6

    Default

    I routinely use MIG wire for TIG on thin gauge sheet steel. Works well and isn't the nightmare that wrecks your puddle like 1/16" is. I'm sure it's mentioned here on the board elsewhere, but if you need a thicker diameter, you can double it over and make a "rod" with your drill & a vise.

  7. #7

    Default

    Quote Originally Posted by cornonda View Post
    I routinely use MIG wire for TIG on thin gauge sheet steel. Works well and isn't the nightmare that wrecks your puddle like 1/16" is. I'm sure it's mentioned here on the board elsewhere, but if you need a thicker diameter, you can double it over and make a "rod" with your drill & a vise.
    Just remember to keep the mig wire off of the floor when you do this to avoid contaminating the metal.

  8. #8

    Default

    Quote Originally Posted by Mr120 View Post
    Just remember to keep the mig wire off of the floor when you do this to avoid contaminating the metal.
    Good point, Mr120. I developed the habit of wiping filler rod before I use it, to help reduce potential contamination.

  9. #9

    Default

    Quote Originally Posted by cornonda View Post
    Good point, Mr120. I developed the habit of wiping filler rod before I use it, to help reduce potential contamination.
    That's definitely a good habit to have. It is infinitely more difficult to thoroughly wipe down a filler rod made of twisted mig wire!

  10. #10
    Join Date
    Nov 2012
    Location
    Whine Country, California
    Posts
    442

    Default

    I use the .035" MIG wire when doing sheet metal work (automotive sheet metal repairs and such). Wiping any wire down that comes off a spool is a good idea. A lot of times I forget to wipe off the "normal" TIG wire that I buy at the LWS, but it is a good practice that I am trying to get in the habit of doing! Obviously if you're welding really thin material, you'll want to get that tungsten sharpened to a needle point, otherwise you can wind 2 or 3 strands of MIG wire together to produce a thicker welding rod for heavier material as others (above) have mentioned.
    Andy
    New Everlast PowerTig 250EX that is begging for me to come up with a few welding projects so it can stretch it's legs. Did someone say aluminum???

    MISC. TOOLS:
    Atlas 618 lathe
    Milwaukee Porta Band with custom made stand
    Dewalt 4-1/2" angle grinder
    Dewalt 14" chop saw

    Strong Hand Nomad portable table
    Juki sewing machine I've had for years (yes I know sewing is for girls)

Similar Threads

  1. welding treated/hardened steel
    By TheGary in forum General Welding Questions
    Replies: 5
    Last Post: 02-24-2017, 02:25 PM
  2. Need some tips on welding 22 ga. steel
    By Ron66 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 09-30-2013, 11:34 PM
  3. Tig Welding Grounding Bar Copper to Steel
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 0
    Last Post: 12-12-2012, 06:04 PM
  4. Replies: 18
    Last Post: 05-26-2012, 08:00 PM
  5. Stainless Steel oxy-acetilene welding, how-to?
    By lwmar in forum General Welding Questions
    Replies: 7
    Last Post: 10-06-2011, 06:12 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •