Steve,
Until you master regular TIG welding, those settings are really meaningless and delay your TIG development.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
How old is the machine? Does it use a pedal with a separate knob on it or is it a more standard pedal?
Everlast 200DX
Everlast PT185
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile
I agree. About 80% of the settings on the machine are not needed for someone who is just starting out.
For learning on Aluminum welding, Set the frequency somewhere between 50-100Hz, set the balance to about the 9 o'clock position, adjust your post flow to something you are comfortable with and leave them all there. Then the only thing you really need to dial in is the current.
Everlast 200DX
Everlast PT185
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile
thanks man.