  1. Default tig welding question

    for example if you're tig welding with a 3/32 tungsten what is best size filler rod to use?

  2. #2

    Default

    Quote Originally Posted by steve1989 View Post
    for example if you're tig welding with a 3/32 tungsten what is best size filler rod to use?
    The tungsten size doesn't matter so much, size the filler for the joint being welded. Here a link to a simple calculator. http://www.millerwelds.com/resources...calculator.php
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3

    Default

    Quote Originally Posted by zoama585 View Post
    The tungsten size doesn't matter so much, size the filler for the joint being welded. Here a link to a simple calculator. http://www.millerwelds.com/resources...calculator.php
    This is also a Droid app.
    I don't know about iPhone.

  4. Default

    There is also an iPhone version available.

Similar Threads

  1. Spot welding question.
    By Brian Ski in forum General Welder Questions
    Replies: 19
    Last Post: 08-18-2014, 12:02 PM
  2. Tube welding question
    By agent4573 in forum General Welding Questions
    Replies: 8
    Last Post: 04-06-2013, 12:01 PM
  3. Welding question
    By Brian Ski in forum General Welding Questions
    Replies: 6
    Last Post: 12-26-2012, 11:49 PM
  4. Welding helmet question
    By Brian Ski in forum General Welding Questions
    Replies: 43
    Last Post: 05-17-2012, 02:22 PM
  5. practice welding question
    By Brian Ski in forum General Welding Questions
    Replies: 22
    Last Post: 05-04-2012, 10:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •