Quote Originally Posted by johnnymg View Post
Thanks again for all of the suggestions. I will order (or pick up) a roll of 0.030" flux cored wire. Will report back with the results of the practice welds.

cheers
JohnG
Don't forget to switch to DCEN for flux core.