    If your wire spool friction knob is too tight, it'll lower the Max inches per minute.

  2. #2

    Default

    Wire speed is a function of amps and amps are dependent upon wire diameter for any given wire speed.

    The 200 amp rating on the i mig 200 is dependent upon wire diameter. For .030 wire, it doesn't get up to 200 amps. Allowing the unit to churn up to 400 ipm for say .035 wire...would result in the machine creating serious overcurrent issues with the unit. The i mig 205 puts out more typically. Measure max wire speed for 30 seconds for best accuracy and most convenience.

    Compare to transformer MIGs...their numbers are theoretical too. Especially look at the duty cycle at which their units are rated. A 140 MIG is usually 15-20% duty cycle at 90 amps....Now how many think that you're going to get the fulll 140 amps for very long at max output? Better question, is how many machines actually get that high combined with true underload wirespeed and maximum wire diameter the unit allows?

    Here's a really good chart I found that explains it and a whole lot more.


    http://www.google.com/url?sa=t&rct=j&q=&esrc=s&source=web&cd=2&ved=0CDkQ FjAB&url=http%3A%2F%2Fwww.airgas.com%2Fdocuments%2 Fpdf%2FMIGWire.pdf&ei=upPeUorQH4nQsATopIH4Ag&usg=A FQjCNE51TwCQFrwJlY9zwb_-psa9MXC-A&bvm=bv.59568121,d.cWc

    Last edited by performance; 01-21-2014 at 02:46 PM.

Similar Threads

  1. Wire Speed Values
    By thegoschman in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 1
    Last Post: 10-19-2016, 10:16 AM
  2. wire feed speed Imig200
    By stretch in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 14
    Last Post: 05-19-2016, 09:48 PM
  3. wire speed accuracy?
    By mts211si in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 20
    Last Post: 11-17-2015, 07:19 PM
  4. I-MIG 250p Low Wire Speed
    By zoama in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 8
    Last Post: 03-05-2012, 12:49 AM
  5. Replies: 26
    Last Post: 02-22-2012, 11:25 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •