I have been using my Imig for a month or so now and find it to be a very smooth welder! Other than the huge rush of argon when the trigger is pulled, due to the hose from the bottle to welder expanding and contracting, i have no issues laying a very satisfactory bead, although im a little curious of the wire speed....
According to the sticker on the wire feed motor itself, it is rated at 12m/min which is equal to 472 inches per minute..... But when turned all the way up, the display only goes a little over 300 inches/min. I did verify the 300in/min and it is very accurate with .035" wire.
The only reason i ask is it makes it difficult to use welder setting cheat sheet to set up the machine for thicker metal. Any insight on this??
Also a side note, the PowerPlasma 80s that i bought over the same phone call as the Imig, is a kick ### machine!!! appropriately dubbed "The Axe" as it cuts through anything FAST!!!!
Thank you Everlast for the savings of not having to go with the over rated blue or red!!!